Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.010 - 0.017 cm/cm
0.010 - 0.017 in/in
Custom Resins Vexel™ 3250 PBT  (discontinued **)
General Purpose Unreinforced; High Flow. Property data for dry as molded samples.Data provided by the manufacturer
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm

@Thickness 3.18 mm
0.015 - 0.017 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125" bars; ASTM D955
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope..
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm

@Thickness 3.18 mm
0.015 - 0.017 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125" bars; ASTM D955
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte..
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm

@Thickness 3.18 mm
0.015 - 0.017 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125"; ASTM D955
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist..
Linear Mold Shrinkage, Transverse 0.016 - 0.017 cm/cm
0.016 - 0.017 in/in
ASTM D955
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Linear Mold Shrinkage, Transverse 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia..
Linear Mold Shrinkage, Transverse 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
LATI Latilub 66-20ST PA66, Silicone/PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). Silicone / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Linear Mold Shrinkage, Transverse 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
LATI Latilub 66-20T PA66, PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic..
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm

@Time 86400 sec
0.015 - 0.017 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA
LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC..
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm

@Time 86400 sec
0.015 - 0.017 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA (Asia Pacific)
LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC..
Linear Mold Shrinkage, Transverse 0.0080 - 0.017 cm/cm
0.0080 - 0.017 in/in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WL004 is a compound based on Polybutylene Terephalate resin containing PTFE.
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm

@Thickness 3.18 mm
0.015 - 0.017 in/in

@Thickness 0.125 in
ASTM D955
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic..
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm

@Thickness 3.18 mm
0.015 - 0.017 in/in

@Thickness 0.125 in
ASTM D955
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and ..
Linear Mold Shrinkage, Transverse 0.010 - 0.017 cm/cm

@Thickness 0.750 - 2.30 mm
0.010 - 0.017 in/in

@Thickness 0.0295 - 0.0906 in
SABIC Method
SABIC Innovative Plastics Valox® 310SE0 PBT
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Linear Mold Shrinkage, Transverse 0.010 - 0.017 cm/cm

@Thickness 0.750 - 2.30 mm
0.010 - 0.017 in/in

@Thickness 0.0295 - 0.0906 in
SABIC Method
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Linear Mold Shrinkage, Transverse 0.010 - 0.017 cm/cm

@Thickness 0.750 - 2.30 mm
0.010 - 0.017 in/in

@Thickness 0.0295 - 0.0906 in
SABIC Method
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm

@Thickness 3.18 mm
0.015 - 0.017 in/in

@Thickness 0.125 in
ASTM D955
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b..
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm

@Thickness 3.18 mm
0.015 - 0.017 in/in

@Thickness 0.125 in
ASTM D955
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK)
KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th..
Linear Mold Shrinkage, Transverse 0.012 - 0.017 cm/cm
0.012 - 0.017 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 745 PBT (Europe-Africa-Middle East)
VALOX 745 is 30% mineral filled PBT injection moulding resin with improved toughness and low warpage. Applications: telephone ringer frames, card racks.
Linear Mold Shrinkage, Transverse 0.011 - 0.017 cm/cm
0.011 - 0.017 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East)
6.5% glass reinforced, Super High Flow, flame retardant PBT.
Linear Mold Shrinkage, Transverse 0.013 - 0.017 cm/cm
0.013 - 0.017 in/in
DIS 294-4
Wellman Wellamid® 42LH-XE-NBK1 Nylon 6, Engineering Grade
All information provided by Wellman Engineered Resins.
Linear Mold Shrinkage, Transverse 0.013 - 0.017 cm/cm
0.013 - 0.017 in/in
DIS 294-4
Wellman Wellamid® 42L-N Nylon 6, General Purpose
All information provided by Wellman Engineered Resins.
Linear Mold Shrinkage, Transverse 0.013 - 0.017 cm/cm
0.013 - 0.017 in/in
DIS 294-4
Wellman Wellamid® 42LN2-NBK2 Nylon 6, General Purpose
All information provided by Wellman Engineered Resins.
Linear Mold Shrinkage, Transverse 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
ISO DIS 294-4
Wellman Wellamid® WE1359 25% Glass Sphere Filled, Toughened Nylon 66
Description: Glass Sphere Filled, Toughened Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.016 - 0.017 cm/cm
0.016 - 0.017 in/in
ASTM D955
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Linear Mold Shrinkage, Transverse 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
LATI Latishield 52/5-07A PP Homopolymer, Steel Fiber Reinforced
EMI shielding product based on Polypropylene homopolymer (PPh). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Linear Mold Shrinkage, Transverse 0.013 - 0.017 cm/cm
0.013 - 0.017 in/in
ISO DIS 294-4
Wellman Wellamid® 42LH-NBK1 General Purpose Nylon 6
Description: General Purpose Nylon 6Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.013 - 0.017 cm/cm
0.013 - 0.017 in/in
DIS 294-4
Wellman Wellamid® 42LH-WBK Nylon 6, Engineering Grade
All information provided by Wellman Engineered Resins.
Copyright © lookpolymers.com All Rights Reserved