Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.017 - 0.018 cm/cm | 0.017 - 0.018 in/in | ASTM D955 |
PolyOne Stat-Tech™ CTX-1125 Natural Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 - 0.018 cm/cm | 0.017 - 0.018 in/in | ASTM D955 |
PolyOne Stat-Tech™ X ST6600-0040 ES FR Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Thickness 3.18 mm |
0.016 - 0.018 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Thickness 3.20 mm |
0.016 - 0.018 in/in @Thickness 0.126 in |
5" x 0.5" x 0.125" bar; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm | 0.016 - 0.018 in/in | |
LATI Latene® 11 MDT05-01 PP Homopolymer Polypropylene homopolymer (PPh) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | |
LATI Later 4-V0HF1 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | |
LATI Latigray 47/1-01 CX/45 PP Copolymer Radiopaque compound based on Polypropylene copolymer (PPc). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | |
LATI Latistat 45/7-02 HDPE Dissipative product based on High density polyethylene (HD-PE). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Thickness 3.18 mm |
0.016 - 0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East) VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® FXV310SK PBT (Europe-Africa-Middle East) LIMITED USE, No New Customers / Applications as of Jan. 2010: VALOX FXV310SK is an unreinforced PBT injection moulding resin with high flow characteristics and containing a metal sparkle Visual FX. .. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® VX3101N PBT (Europe-Africa-Middle East) VALOX VX3101N is an unreinforced PBT injection moulding resin, with excellent flow properties, good hydrolitical stability and chemical resistance. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.018 cm/cm @Thickness 3.20 mm |
0.016 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | DIS 294-4 |
Wellman Wellamid® GSF1849-N1 Nylon 66, 40% Glass Sphere/Fiber Reinforced Developmental productAll information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | DIS 294-4 |
Wellman Wellamid® MRT1487 BK Nylon 66, 32% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | DIS 294-4 |
Wellman Wellamid® MRT1487 N Nylon 66, 32% Mineral Reinforced, Impact Modified All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | |
LATI Later 4-V0 PBT, Flame Retardant Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide freeAvailability: Africa & Middle East; Asia Pacific; Europe; L.. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | |
LATI Latimass 53/11-02 D030 PP Homopolymer, Impact Modified Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East) VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.018 cm/cm | 0.0090 - 0.018 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East) VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI.. |