Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.017 - 0.023 cm/cm | 0.017 - 0.023 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1615-BK Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1482-BK High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1606-N Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.023 cm/cm | 0.0080 - 0.023 in/in | Flame Bar; ASTM D955 |
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU) A novel copolymer that is strong yet flexible with proven biocompatibility and biostability
Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional.. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | DIS 294-4 |
Wellman Wellamid® 22L-NBK1/WE-1434 Nylon 66, Engineering Grade All information provided by Wellman Engineered Resins. |