Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm @Thickness 6.35 mm |
0.0030 - 0.0040 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® J-68/20/E/SD/HM Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled, with static dissipation Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm @Thickness 1.60 mm |
0.0010 - 0.0040 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax PBT 4140-201D 40% Glass Fiber Filled Product Description: A glass fiber 40% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm @Thickness 1.60 mm |
0.0010 - 0.0040 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax PBT 5130-104 30% Glass Fiber Filled CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm @Thickness 6.35 mm |
0.0030 - 0.0040 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® J-68/20/E/SD Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled, with static dissipation Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0025 - 0.0040 cm/cm @Thickness 6.35 mm |
0.0025 - 0.0040 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® J-68/25/E/SD Polypropylene Copolymer, 25% Glass Fiber Reinforced, Chemically coupled, with static dissipation Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0010 - 0.0040 cm/cm @Thickness 1.60 mm |
0.0010 - 0.0040 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP ABS/PBT 7320H-104 20% Glass Fiber Filled Product Description: A 20% glass fiber reinforced injection molding grade. Characteristics:Low warp age and excellent dimensionally stable Excellent electrical property Excellent mechanic and chemi.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 80°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 80°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 1.00 mm |
0.0020 - 0.0040 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-402 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 1.00 mm |
0.0020 - 0.0040 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 1.00 mm |
0.0020 - 0.0040 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 1.00 mm |
0.0020 - 0.0040 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 1.00 mm |
0.0020 - 0.0040 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-669VGB Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 1.00 mm |
0.0020 - 0.0040 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 80°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 80°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm @Thickness 6.35 mm |
0.0030 - 0.0040 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® J-62/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 1.60 mm |
0.0020 - 0.0040 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP PBT 3040-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 80°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |