Polymer Property : Linear Mold Shrinkage = 0.014 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.014 cm/cm

@Thickness 6.40 mm
0.014 in/in

@Thickness 0.252 in
Flow; DAM
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66  (Unverified Data**)
Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.014 cm/cm

@Thickness 6.40 mm
0.014 in/in

@Thickness 0.252 in
Transverse; DAM
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66  (Unverified Data**)
Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.014 cm/cm

@Thickness 6.35 mm
0.014 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.014 - 0.016 cm/cm

@Thickness 6.35 mm
0.014 - 0.016 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.014 - 0.016 cm/cm

@Thickness 6.35 mm
0.014 - 0.016 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.014 - 0.020 cm/cm

@Thickness 1.60 mm
0.014 - 0.020 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 4115-104D 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.014 - 0.020 cm/cm

@Thickness 1.60 mm
0.014 - 0.020 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 3015-201 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.014 - 0.018 cm/cm

@Thickness 3.00 mm
0.014 - 0.018 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.014 - 0.018 cm/cm

@Thickness 3.00 mm
0.014 - 0.018 in/in

@Thickness 0.118 in
DAM
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (Conditioned)
Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo.
Linear Mold Shrinkage 0.014 - 0.018 cm/cm

@Thickness 3.00 mm
0.014 - 0.018 in/in

@Thickness 0.118 in
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (DAM)
Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo.
Linear Mold Shrinkage 0.014 - 0.018 cm/cm

@Thickness 3.00 mm
0.014 - 0.018 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.014 cm/cm

@Thickness 3.20 mm
0.014 in/in

@Thickness 0.126 in
Flow
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT
Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide..
Linear Mold Shrinkage 0.014 - 0.020 cm/cm

@Thickness 1.60 mm
0.014 - 0.020 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.014 - 0.020 cm/cm

@Thickness 1.60 mm
0.014 - 0.020 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 3015-104 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.014 - 0.020 cm/cm

@Thickness 1.60 mm
0.014 - 0.020 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 4115-201D 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..