Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 100 g/10 min @Load 21.6 kg, Temperature 190 °C |
100 g/10 min @Load 47.6 lb, Temperature 374 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® A 85 P 4722 TPU-Polyester Introduction: IROGRAN A 85 P 4722 is a halogen-free thermoplastic- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are good microbial resista.. |
|||
Melt Index of Compound | 100 g/10 min @Load 2.16 kg, Temperature 190 °C |
100 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-9810 NT 7 is produced using UNIPOL™ PE process technology and is supplied in pellet form. This resin is specifically designed as a carrier resin for color concentrates and other masterbat.. |
|||
Melt Index of Compound | 100 g/10 min @Load 2.16 kg, Temperature 190 °C |
100 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow DNDB-1077 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-1077 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |