Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 23 g/10 min @Load 5.00 kg, Temperature 230 °C |
23 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs T00 ABS, Transparent Information provided by Polykemi AB |
|||
Melt Index of Compound | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Melt Index of Compound | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Asia Pacific) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Melt Index of Compound | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Melt Index of Compound | 23 g/10 min @Load 2.16 kg, Temperature 275 °C |
23 g/10 min @Load 4.76 lb, Temperature 527 °F |
ISO 1133 |
Polykemi AB SCANBLEND P AP2060 F30 PBT/ASA, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® BPL1000 PC Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Europe-Africa-Middle East) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HF1140R PC High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1 PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1R PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount o.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPF1 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS1 PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS1R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Cont.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HPS1S PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® LUX7189 PC (Europe-Africa-Middle East) Lexan* LUX7189 is an injection moldable, high light reflectance FR grade. Contains non-brominated, non-chlorinated flame retardant systems. |
|||
Melt Index of Compound | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Asia Pacific) CY5100 is a Flame retardant PC blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HF1140 PC Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this.. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1R PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Melt Index of Compound | 23 g/10 min @Load 3.80 kg, Temperature 230 °C |
23 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical IF870S PMMA, General Purpose Grade for Injection Molding Highest flowability of all gradesFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface hardness and coloring propertySuperior electrical resistance and mecha.. |
|||
Melt Index of Compound | 23 g/10 min @Load 5.00 kg, Temperature 280 °C |
23 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications. |
|||
Melt Index of Compound | 23 g/10 min @Load 5.00 kg, Temperature 280 °C |
23 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL N190X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications. |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Europe-Africa-Middle East) 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Melt Index of Compound | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Europe-Africa-Middle East) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |