Physical Properties Metric English Comments
Viscosity 1.60e+6 cP
1.60e+6 cP
B
Shin-Etsu Silicones LIMSâ„¢ KEG2000-40A/B Elastomer
KEG2000-40 is a fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to..
Viscosity 1.60e+6 cP
1.60e+6 cP
A
Shin-Etsu Silicones LIMSâ„¢ KEG2000-60A/B Elastomer
KEG2000-60 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum..
Viscosity 1.60e+6 cP
1.60e+6 cP
B
Shin-Etsu Silicones LIMSâ„¢ KEG2000-60A/B Elastomer
KEG2000-60 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum..
Viscosity 1.60e+6 cP
1.60e+6 cP
B
Shin-Etsu Silicones LIMSâ„¢ KEG2000-50A/B Elastomer
KEG2000-50 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum..
Viscosity 1.60e+6 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
1.60e+6 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Bynel® 41E556 Anhydride-Modified LLDPE Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi..
Viscosity 1.60e+6 cP

@Temperature 260 °C
1.60e+6 cP

@Temperature 500 °F
Melt Viscosity; DSM method
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
Viscosity 1.60e+6 - 2.80e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
1.60e+6 - 2.80e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Viscosity 1.60e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
1.60e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Viscosity 1.60e+6 cP

@Shear Rate 100 1/s,
Temperature 190 °C
1.60e+6 cP

@Shear Rate 100 1/s,
Temperature 374 °F
ATOFINA research test
Total Lacqtene® 2001 TBK 46 HDPE pipe  (discontinued **)
LACQTENE® 2001 TBK 46 is a high density polyethylene produced by the gas phase polymerization process. LACQTENE® 2001 TBK 46 is a black compound especially developed for pressure pipe for gas and ..
Viscosity 1.60e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
1.60e+6 - 2.00e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..