Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 70 - 130 cP | 70 - 130 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-120 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Max. toluene solubility, MC solubleExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Use.. |
|||
Viscosity | 70 - 130 cP | 70 - 130 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-120L TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Max. toluene solubility, MC solubleExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Use.. |
|||
Viscosity | 100 - 130 cP | 100 - 130 cP | uncured coating |
Master Bond UV15SP-1 Low Viscosity, UV Curable System Description: Master Bond UV15SP-1 is a new one component, high strength UV curable epoxy resin based polymer system for bonding, sealing, & coating with high performance properties. It is a 100% rea.. |
|||
Viscosity | 70 - 130 cP | 70 - 130 cP | |
3M Scotch-Weld™ CA8 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Slower setting than CA7 and excellent adhesion to metals, and plastics and rubbers. Meets CID A-A-3.. |