Physical Properties Metric English Comments
Viscosity 12000 - 16000 cP
12000 - 16000 cP
ND Industries 440 High pressure Sealant
Pneumatic and hydraulic sealant fluid, for power and gas system connections
Viscosity 10000 - 16000 cP
10000 - 16000 cP
Of hardener at 25C
Resin Technology Group TIGA 101-EX Five-Minute Epoxy Adhesive
1 part resin to 1 part hardener.TIGA 101-EX is an exceptional epoxy formulation, recommended for lower temperature or wet industrial bonding applications where fast curing is required. This clear, t..
Viscosity 8000 - 16000 cP

@Temperature 175 °C
8000 - 16000 cP

@Temperature 347 °F
Automatic orifice Viscosity
Cookson Group Plaskon® 3400 Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A reduced-stress epoxy molding compound for the encapsulation of a variety of semiconductor devices ranging from small lead count..
Viscosity 6000 - 16000 cP
6000 - 16000 cP
Huntsman AroCy XU 71787.07 L Cyanate Ester
Comments/Applications: Toughened Dicyclopentadiene based cyanate ester resin.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Viscosity 14000 - 16000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
14000 - 16000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2050303D1 Fine Line Printing Ink
Silver Ink has been designed for fine line printing. It is capable of printing down to 50 micron line and spaces within a production environment. Under laboratory conditions, finer lines and spaces ..
Viscosity 11000 - 16000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
11000 - 16000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2061103D7 Lead free Silver Zinc Basecoat Paste
This product is a lead-free version of C70709D22. The ink is designed as a screen printing ink for coating Barium Titanate PTC ceramics as the base layer of a two part system. The dried film should..
Viscosity 14000 - 16000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
14000 - 16000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials D2070423D5 Polymer Dielectric
Grey colored screen printable polymer dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode. The formulation i..
Viscosity 12000 - 16000 cP

@Temperature 23.0 °C
12000 - 16000 cP

@Temperature 73.4 °F
20 rpm
Epoxy Technology EPO-TEK® OE120 Two Component Epoxy
Material Description: A two component, opaque epoxy, designed for fiber optics packaging applications. It is a black-colored version of EPO-TEK 353ND-T. It has a high Tg for resisting elevated ope..
Viscosity 12000 - 16000 cP
12000 - 16000 cP
uncured
Atom Adhesives AA-BOND FDA2 Epoxy Adhesive
AA-BOND FDA2 is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and recei..
Viscosity 7000 - 16000 cP
7000 - 16000 cP
Base
3M Scotch-Weld™ DP270 Black Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M