Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 19 cP @Temperature 23.0 °C |
19 cP @Temperature 73.4 °F |
Shear gradient 250 s^-1 |
Solvay Specialty Polymers Diofan® A602 Polyvinylidene Chloride (PVDC)
(discontinued **) DIOFAN® A602 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. It features strong barrier prop.. |
|||
Viscosity | 19 cP | 19 cP | |
Asahi Glass Fluon® AD936 PTFE Aqueous Dispersion Fluon®PTFE aqueous dispersions are useful for glass cloth coating, metal coating, binder, additive in resin, feedstock of heat resistive paint ,etc.Information provided by Asahi Glass Company, Inc... |