Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 4000 cP | 4000 cP | |
Resinlab® CYNERGY CA6209 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Viscosity | 4000 cP | 4000 cP | |
Resinlab® CYNERGY CA6309 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV615 Clear General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
|
Momentive Performance Materials RTV656 Clear Extreme Low Temperature Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | 30% solid in Anone |
Taiwan Sheen Soon Sheenthane® A7710 TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
Viscosity | 4000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
4000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7020-1000 TPE Product Description: StarMediflex P 7020-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | |
Master Bond EP46HT Epoxy Adhesive for Structural Bonding Description: Master Bond System EP46HT is a newly formulated two component high performance heat resistant epoxy resin system with excellent mechanical strength and chemically resistant properties f.. |
|||
Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
Mixed (10 rpm) |
Tra-Con Tra-Cast 3108 General Purpose Epoxy Casting Compound TRA-CAST 3108 is a low viscosity two-part formulation recommended for underfill and encapsulating applications where the combination of good mechanical thermal and electrical properties are required.. |
|||
Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
Mixed (10 rpm) |
Tra-Con Tra-Cast 3113 General Purpose Epoxy Casting Compound TRA-CAST 3113 is a low viscosity two-part formulation recommended for general purpose electrical potting and encapsulating applications where the combination of good mechanical thermal and electrica.. |
|||
Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Cast FS330 Fire Retardant Long Pot Life Epoxy Casting Compound TRA-CAST FS330 is a low viscosity, long pot life, thermally conductive casting compound which passes UL 94 V-O. It is recommended for rigid potting, laminating, transformer encapsulating, filament w.. |
|||
Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Stycast® 2057/9 Two-Component General Purpose Encapsulant Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as .. |
|||
Viscosity | 4000 cP @Temperature 25.0 °C |
4000 cP @Temperature 77.0 °F |
|
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Viscosity | 4000 - 8000 cP @Temperature 23.0 °C |
4000 - 8000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® B9021 Epoxy Paste Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta.. |
|||
Viscosity | 4000 - 7000 cP | 4000 - 7000 cP | |
Epoxyset Epoxibond EB-135 Unfilled Epoxy Adhesive A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries. EB-135 has excellent bond strength to various substrat.. |
|||
Viscosity | 4000 - 5000 cP | 4000 - 5000 cP | |
Epoxyset Epoxiohm EO-23M Electrically Conductive Epoxy Adhesive EO-23M is an electrically conductive, low viscosity silver-filled epoxy adhesive. Used for hybrid / micro-electronic adhesive including die-attach and substrate attach for Rf and Microwave devices.I.. |
|||
Viscosity | 4000 cP | 4000 cP | STD |
Dymax 602 Structural Adhesive Structural Adhesives for Rugged Bonding, Sealing, Tacking and Potting in SecondsMulti-Cure® 600 Series products are rapid setting adhesives that cure by UV light, activator or heat. These products .. |
|||
Viscosity | 4000 cP | 4000 cP | |
Dymax 955 Potting and Encapsulation Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 955 Potting and Encapsulation AdhesiveHigh strength with superior adhesion to steel, aluminum and glass. Cure Type: .. |
|||
Viscosity | 4000 cP | 4000 cP | Mixed |
Aremco Aremco-Bond™ 2315X High Temperature Epoxide Potting Compound Improved Crack Resistance & Bond Strength. High Temperature Resistance, Thermally Conductive, Low Viscosity. |
|||
Viscosity | 4000 cP | 4000 cP | uncured |
Atom Adhesives AA-BOND F123 Epoxy Adhesive AA-BOND F123 is a low viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating single or multi.. |
|||
Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | 50-6 |
Abatron AboCast 50-6/AboCure 50-12 Epoxy Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Colorless. Shelf life is 12+ months. |
|||
Viscosity | 4000 cP | 4000 cP | |
Abatron AboCast 7703-21/AboCure 7703-21 (A) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Viscosity | 4000 cP | 4000 cP | "A" component |
ACC QSil 550SB QSI Quantum Silicones Self-Priming Silicone Potting Material QSil 550SB is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repair.. |
|||
Viscosity | 4000 - 5.00e+7 cP @Shear Rate 0.100 - 11000 1/s |
4000 - 5.00e+7 cP @Shear Rate 0.100 - 11000 1/s |
Average value: 1.53e+6 cP Grade Count:111 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |
|||
Viscosity | 4000 cP | 4000 cP | QSil 216A |
ACC QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber QSil 216 is a two-part, clear, liquid silicone which will cure at room temperature or at elevated temperatures. It has a low viscosity, which allows for ease of flow around complex parts, providing .. |
|||
Viscosity | 4000 cP | 4000 cP | Part B (Polyol), RVT, #3, 20 rpm; TM R050-12 |
Resinlab® UR3001HP Clear Urethane Encapsulant Resinlab™ UR3001HP Clear is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Clear provides excellent e.. |
|||
Viscosity | 4000 cP | 4000 cP | Mixed |
Resinlab® UR3005 Two Part Urethane Elastomer Resinlab™ UR 3005 is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 provides excellen.. |