Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 500 - 700 cP | 500 - 700 cP | |
ND Industries SuperGlue Ethyl 344 Medium viscosity, general purposeMeets military spec Mil-A-46050C Type II Class III |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Huntsman Araldite GY 506 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 172 to 185. Max color is 1.Comments/Applications: GY 6010 modified with RD-1 (BGE) - a monofunctional reactive diluent. Good impregnation and maximum filler loading... |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Huntsman Araldite GY 507 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 180 to 192. Max color is 3.Comments/Applications: GY 6010 modified with DY 023 (CGE) - a monofunctional reactive diluent. General purpose, modified resin. Very low .. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Huntsman Araldite GY 509 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 189 to 200. Max color is 1.Comments/Applications: GY 6010 cut with DY 027 (Epoxide 7). Longer pot life, lower exotherm. General purpose low viscosity resin.Data pro.. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | A component |
Taiwan PU Corporation TPL-THANE 5085-A/B High Pressure Urethane Spraying Elastomer 5085-A is a high reactivity polyethamine content extender. 5085-B is a methylene diphenyklene dissocyanate(MDI). They make up the third generation high pressure urethane spraying elastomer. It ha.. |
|||
Viscosity | 350 - 700 cP | 350 - 700 cP | LVTDV-I-A3 V50; RP-0596 |
Solvay RHODOLINE® DF 540 Surfactant Description: Highly effective white oil defoamer for latex processing.Identification: DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© DF 540 is a general purpose silicone-free, high a.. |
|||
Viscosity | 600 - 700 cP @Temperature 23.0 °C |
600 - 700 cP @Temperature 73.4 °F |
|
Master Bond UV10FL-1 Flexibilized One Component UV Curable Adhesive Master Bond UV10FL-1 is a one component UV curable modified compounds, ready for use as supplied, for high performance casting and bonding applications. UV10FL-1 is a flexibilized system; it exhibit.. |
|||
Viscosity | 150 - 700 cP @Temperature 190 °C |
150 - 700 cP @Temperature 374 °F |
542-130 |
Westlake Epolene® E-25 Chemically Modified Polypropylene, Maleation Processed Product Description: Epolene E-25 is a maleic anhydride grafted polypropylene recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emul.. |
|||
Viscosity | 150 - 700 cP @Temperature 190 °C |
150 - 700 cP @Temperature 374 °F |
542-111 |
Westlake Epolene® E-43 Chemically Modified Polypropylene, Maleation Processed Product Description: Epolene E-43 is a maleic anhydride grafted polypropylene recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emul.. |
|||
Viscosity | 500 - 700 cP @Temperature 25.0 °C |
500 - 700 cP @Temperature 77.0 °F |
Initial Mix Viscosity (Hoeppler) |
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process. |
|||
Viscosity | 350 - 700 cP | 350 - 700 cP | Part B |
Master Bond EP30M4 Chemically Resistant Two Component Epoxy System Master Bond Polymer System EP30M4 is a two component epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weight. EP30M4 resi.. |
|||
Viscosity | 300 - 700 cP | 300 - 700 cP | NOV QC 020 |
Lubrizol ESTANE® 5701F1 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 441 - 700 cP @Temperature 25.0 °C |
441 - 700 cP @Temperature 77.0 °F |
|
Esstech X-167-0470 Glass Ionomer Cement Liquid Our GIC liquid works well when paired with an alumino-fluoro-silicate glass filler. The combination leads to a quick, easy-to-use composite material. Listed on the Toxic Substance Control Act List... |
|||
Viscosity | 550 - 700 cP @Temperature 35.0 °C |
550 - 700 cP @Temperature 95.0 °F |
Dynamic viscosity |
C.O.I.M. PLAXTER® P 70 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of conveyor belt manufacturing as well as in the field of synthetic leathers.Information provided by P.A.T. Products, Inc. |
|||
Viscosity | 520 - 700 cP @Temperature 25.0 °C |
520 - 700 cP @Temperature 77.0 °F |
|
ACC EP Primer 28 EPI Engineered Polymers Aromatic polyisocyanate Prepolymer EP Primer 28 is a polyisocyanate prepolymer based on diphenylmethane diisocyanate (MDI). As corrosion-resistant primers, coatings based on EP Primer 28 polyisocyanate can be formulated to contain z.. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | blended |
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Viscosity | 400 - 700 cP | 400 - 700 cP | |
Aremco Ceramacoat™ 845-GRY High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, gray coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu.. |
|||
Viscosity | 400 - 700 cP | 400 - 700 cP | |
Aremco Ceramacoat™ 845-WHT High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, white coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadi.. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 350 - 700 cP | 350 - 700 cP | Part B |
Master Bond EP30M4LV Chemically Resistant, Low Viscosity Adhesive Description: Master Bond EP30M4LV is a two component, low viscosity epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weig.. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Huntsman Araldite GY 9667 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 196 to 212. Max color is 2.Comments/Applications: GY 6020 modified with DY 025 (Epoxide 8) for less crystallization and improved elongation. High solids and solvent .. |