Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 770 cP | 770 cP | |
Dow ISONATE™ 181 MDI Prepolymer ISONATE™ 181 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with sufficient glycol to allow easy handling down to 80°F. This medium-viscos.. |
|||
Viscosity | 770 cP | 770 cP | |
Dow ISONATE™ 181 MDI Prepolymer ISONATE™ 181 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with sufficient glycol to allow easy handling down to 80°F. This medium-viscos.. |
|||
Viscosity | 770 cP | 770 cP | Prepolymer [Part A]; 3M Method TM-173 |
3M Scotchcast™ 2136 Potting Kit The 3M Scotchcast Potting Kit 2136 is designed to provide protection against corrosion and possible deteriorating effects of fresh swimming pool or fountain water and sunlight by reliably encapsulat.. |