Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 20000 - 80000 cP
20000 - 80000 cP
Lord Adhesives 206 Long Working Time Acrylic Adhesive
Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f..
Viscosity 10000 - 80000 cP
10000 - 80000 cP
Hardener
Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic Adhesive
Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic AdhesiveLord 660 Acrylic Adhesive bonds FRP (fiber-reinforced plastics) with minimal surface preparation. Lord 660 can cross-bond FRP to m..
Viscosity 50000 - 80000 cP
50000 - 80000 cP
B
ITW Plexus Plexusâ„¢ MA420FS Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, very fast curing.Information provided by Illinois Tool Works.
Viscosity 50000 - 80000 cP
50000 - 80000 cP
B
ITW Plexus Plexusâ„¢ MA820 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent for structural bonding of surface metals with no surface preparation.Information provide..
Viscosity 50000 - 80000 cP
50000 - 80000 cP
B
ITW Plexus Plexusâ„¢ MA822 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Designed for structural bonding of metals without primers.Information provided by Illinois Tool Wo..
Viscosity 40000 - 80000 cP
40000 - 80000 cP
ASTM D803
SK Chemicals SKYTHANE® U0351C Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Viscosity 40000 - 80000 cP
40000 - 80000 cP
ASTM D803
SK Chemicals SKYTHANE® U1753C Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Viscosity 40000 - 80000 cP
40000 - 80000 cP
ASTM D803
SK Chemicals SKYTHANE® US130J Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Viscosity 70000 - 80000 cP
70000 - 80000 cP
Master Bond EP51FL-1 Rapid Curing Cryogenic Two Component Epoxy
Master Bond Polymer System EP51FL-1 is a two component highly flexible epoxy resin system for high performance bonding sealing and coating. Although most flexiblilized epoxy formulations are very sl..
Viscosity 60000 - 80000 cP
60000 - 80000 cP
Master Bond LED401LV One Component, Moderate Viscosity LED Curable System
Master Bond LED401LV is a very special, one part LED type system that will cure when exposed to a light source emitting 405 nm wavelength and where the presence of any UV light is minimal or inciden..
Viscosity 70000 - 80000 cP

@Temperature 23.0 °C
70000 - 80000 cP

@Temperature 73.4 °F
Master Bond EP21TDC-2 Highly Flexible Cryogenic Epoxy Compound
Master Bond Polymer System EP21TDC-2 is a two component highly flexible epoxy resin compound for high performance bonding, sealing, coating and encapsulation. It is formulated to cure fully at ambie..
Viscosity 70000 - 80000 cP

@Temperature 23.0 °C
70000 - 80000 cP

@Temperature 73.4 °F
Master Bond EP34 Room Temperature Curing Two Component Epoxy System
Master Bond Polymer System EP34 is a unique room temperature curing two component epoxy compound for high temperature potting and encapsulating applications. Adhesion to metals, glass, ceramics, woo..
Viscosity 70000 - 80000 cP

@Temperature 23.0 °C
70000 - 80000 cP

@Temperature 73.4 °F
Master Bond EP35 High Temperature Resistant Two Component Epoxy System
Master Bond Polymer Adhesive EP35 is a unique, room temperature curing, two component epoxy adhesive for high temperature bonding applications. Master Bond Polymer Adhesive EP35 produces high stren..
Viscosity 20000 - 80000 cP
20000 - 80000 cP
dynamic
Dow Corning Q2-7406 ADHESIVE
Dow Corning® Q2-7406 Adhesive is a polydimethylsiloxane gum and resin dispersion; provides excellent high temperature properties with adhesion to 288C (550F).Information provided by Dow Corning
Viscosity 30000 - 80000 cP
30000 - 80000 cP
dynamic
Dow Corning Q2-7735 ADHESIVE
Dow Corning® Q2-7735 Adhesive is a polydimethylsiloxane gum and resin dispersion, and provides high tack combined with good adhesion.Information provided by Dow Corning
Viscosity 40000 - 80000 cP
40000 - 80000 cP
3M Scotch-Weld™ EC-1469 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1469 is a one-part, 100% solids, thermosetting liquidInformation provided by 3M
Viscosity 40000 - 80000 cP
40000 - 80000 cP
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Viscosity 40000 - 80000 cP
40000 - 80000 cP
Aremco Ceramabond™ 835-MB High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Viscosity 40000 - 80000 cP
40000 - 80000 cP
Aremco Ceramabond™ 668 High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Viscosity 60000 - 80000 cP
60000 - 80000 cP
Aremco Ceramacoat™ 512-N High Temperature Potting & Casting Material Silica
Viscous, off-white paste for circuit breakers, power resistors and solenoids to 240°F (1316°C)
Viscosity 24000 - 80000 cP
24000 - 80000 cP
Thixotropic
Loctite® 577 Coarse Threads Thread Sealant
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p..