Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.470 g/cc | 0.0170 lb/in³ | |
NanoAmor 95%, OD/WT/L: 20-40/5-15 nm/0.5-5 um Multi-Walled Carbon Nanotubes ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh.. |
|||
Apparent Bulk Density | 0.470 - 0.620 g/cc | 0.0170 - 0.0224 lb/in³ | Average value: 0.551 g/cc Grade Count:9 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Apparent Bulk Density | 0.470 - 0.470 g/cc | 0.0170 - 0.0170 lb/in³ | ASTM D792 |
LyondellBasell Montell 1900 UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transferAp.. |
|||
Apparent Bulk Density | 0.470 - 0.470 g/cc | 0.0170 - 0.0170 lb/in³ | ASTM D792 |
LyondellBasell Montell 1900CM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of fraction, good chemical resistance, low odor and taste transfer, .. |
|||
Apparent Bulk Density | 0.470 - 0.470 g/cc | 0.0170 - 0.0170 lb/in³ | ASTM D792 |
LyondellBasell Montell 1900H UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, .. |
|||
Apparent Bulk Density | 0.470 - 0.470 g/cc | 0.0170 - 0.0170 lb/in³ | ASTM D792 |
LyondellBasell Montell 1900LCM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transferAp.. |
|||
Apparent Bulk Density | 0.470 g/cc | 0.0170 lb/in³ | ISO 60 |
SolVin 271DF Polyvinyl Chloride General Purpose - Plasticized Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized and semi-rigid profiles and pipes
- blowing of plasticized films
Calendering : opaque or transparent, plasticized and semi-r.. |
|||
Apparent Bulk Density | 0.470 - 0.530 g/cc | 0.0170 - 0.0191 lb/in³ | ISO 60:1977 |
BorsodChem ONGROVIL S-494 Suspension PVC-Resin S-494 is a suspension type PVC homopolymer of high molecular mass. It is characterized by a porous particle structure and a narrow range of particle size. It retains its excellent pourability even a.. |
|||
Apparent Bulk Density | 0.470 - 0.530 g/cc | 0.0170 - 0.0191 lb/in³ | ISO 60:1977 |
BorsodChem ONGROVIL S-5070 Suspension PVC-Resin S-5070 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It r.. |
|||
Apparent Bulk Density | 0.470 - 0.780 g/cc | 0.0170 - 0.0282 lb/in³ | Average value: 0.549 g/cc Grade Count:11 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Apparent Bulk Density | 0.470 g/cc | 0.0170 lb/in³ | ISO 60 |
SolVin 275SC Polyvinyl Chloride General Purpose - Plasticized Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized and semi-rigid profiles and pipes
Calendering : opaque or transparent, plasticized and semi-rigid films and sheets.Informati.. |