Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.490 - 0.510 g/cc | 0.0177 - 0.0184 lb/in³ | ASTM D792 |
LyondellBasell Montell HB312CM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, .. |
|||
Apparent Bulk Density | 0.490 - 0.510 g/cc | 0.0177 - 0.0184 lb/in³ | ASTM D792 |
LyondellBasell Montell HB320CM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, .. |
|||
Apparent Bulk Density | 0.490 g/cc | 0.0177 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Apparent Bulk Density | 0.490 g/cc | 0.0177 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Durez® 31735 Phenolic, Injection Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Apparent Bulk Density | 0.490 g/cc | 0.0177 lb/in³ | |
Sumitomo Bakelite North America 2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Am.. |
|||
Apparent Bulk Density | 0.490 g/cc | 0.0177 lb/in³ | |
Arkema Group Lacovyl® GS 1300 PVC LACOVYL GS 1300 is a vinyl chloride homopolymer produced by a suspension polymerization process.Characteristics : Viscosity index (ISO 1628-2):124 ml/g,(K value:70). Apparent density (ISO 60):0.49 g.. |