Physical Properties Metric English Comments
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
ISO 60
Raschig Group DECAL® 1760 Phenolic
Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an..
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
ISO 60
Raschig Group MELOPAS® 156 MF Melamine
Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200..
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
ISO 60
Raschig Group MELOPLAS® 3025 MF
Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu..
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
ISO 60
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Apparent Bulk Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
ISO 60
Raschig Group SURAPLAST 54 UPA
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
Apparent Bulk Density 0.450 - 0.800 g/cc
0.0163 - 0.0289 lb/in³
Average value: 0.584 g/cc Grade Count:16
Overview of materials for Polyvinyl Chloride - Polyvinyl Acetate Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Chloride - Polyvinyl Acetate Copolymer". Each property range of values reported is minimum and..
Apparent Bulk Density 0.740 - 0.800 g/cc
0.0267 - 0.0289 lb/in³
Average value: 0.770 g/cc Grade Count:4
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma..
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
Domo Domamid® 24 Polyamide 6
DOMAMID® 24 are a low viscous Polyamide 6 pellets produced from Caprolactam by polymerization. Applications: Textile yarn extrusionCompounding Injection moulding Information provided by Domo
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
Domo Domamid® 24 T Polyamide 6
DOMAMID® 24 T are a low viscous Polyamide 6 pellets produced from Caprolactam by polymerization. Domamid T products are special textile grades with a high uniformity of relative viscosity and Amino..
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
Domo Domamid® 24 T-HS Polyamide 6
DOMAMID® 24 T-HS are a low-viscous Polyamide 6 pellets produced from Caprolactam by polymerization. Domamid®-T-products are special textile grades with a high uniformity of relative viscosity and ..
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
Domo Domamid® 2403 T-HS Polyamide 6
DOMAMID® 2403 T-HS are a low-viscous Polyamide 6 pellets produced from Caprolactam by polymerization. Domamid®-T-products are special textile grades with a high uniformity of relative viscosity an..
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
Domo Domamid® 28 Polyamide 6
DOMAMID® 28 are Polyamide 6 pellets produced from Caprolactam by polymerization.Applications: Textile yarn extrusionCompounding Injection moulding Information provided by Domo
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
Domo Domamid® 32 Polyamide 6
DOMAMID® 32 are Polyamide 6 pellets with a higher viscosity produced from Caprolactam by polymerization.Applications: Standard quality for production of monofilaments and fishing netsInformation pr..
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
Domo Domamid® 33 Polyamide 6
DOMAMID® 33 are Polyamide 6 pellets with a higher viscosity produced from Caprolactam by polymerization. Applications: Standard quality for production of monofilaments and fishing netsInformation p..
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
Domo Domamid® 34 Polyamide 6
DOMAMID® 34 are Polyamide 6 pellets with a higher viscosity produced from Caprolactam by polymerization. Applications: Standard quality for production of monofilaments and filmsInformation provided..
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
Domo Domamid® 27 Polyamide 6
DOMAMID® 27 are Polyamide 6 pellets produced from Caprolactam by polymerization.Applications: Textile yarn extrusionCompounding Injection moulding Information provided by Domo
Apparent Bulk Density 0.680 - 0.800 g/cc
0.0246 - 0.0289 lb/in³
IS 867-1963
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded
Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg..
Apparent Bulk Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
IS 867-1963
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color..
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
ISO 60
Raschig Group DECAL® 152CL Phenolic
Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet..
Apparent Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
ISO 60
Raschig Group RESINOL® 400 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Apparent Bulk Density 0.500 - 0.800 g/cc
0.0181 - 0.0289 lb/in³
Average value: 0.655 g/cc Grade Count:11
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..
Apparent Bulk Density 0.425 - 0.800 g/cc
0.0154 - 0.0289 lb/in³
Average value: 0.650 g/cc Grade Count:12
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..