Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.470 - 0.470 g/cc | 0.0170 - 0.0170 lb/in³ | ASTM D792 |
LyondellBasell Montell 1900 UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transferAp.. |
|||
Apparent Bulk Density | 0.470 - 0.470 g/cc | 0.0170 - 0.0170 lb/in³ | ASTM D792 |
LyondellBasell Montell 1900CM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of fraction, good chemical resistance, low odor and taste transfer, .. |
|||
Apparent Bulk Density | 0.470 - 0.470 g/cc | 0.0170 - 0.0170 lb/in³ | ASTM D792 |
LyondellBasell Montell 1900H UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transfer, .. |
|||
Apparent Bulk Density | 0.470 - 0.470 g/cc | 0.0170 - 0.0170 lb/in³ | ASTM D792 |
LyondellBasell Montell 1900LCM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of friction, good chemical resistance, low odor and taste transferAp.. |