Physical Properties | Metric | English | Comments |
---|---|---|---|
API Gravity | 38.5 ° | 38.5 ° | |
ChevronTexaco Oil Rust Proof Texaco Rust Proof Oil delivers value through:Good short-term rust protection — Low viscosity oil provides complete coverage of metal surfaces for maximum protection against oxidation and corrosion... |