Polymer Property : Melt Flow = 0.28 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.28 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.28 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition G; ASTM D1238
Global D-2022 Low Density Polyethylene, Film Extrusion Grade  (discontinued **)
Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-bagsMeets FDA requirements as listed in food additives regulation 21 CFR 117.1520 fo..
Melt Flow 0.28 g/10 min
0.28 g/10 min
Condition 190/2.16; ASTM D1238
Chevron Phillips Marlex® HHM TR-140 Polyethylene, Film Grade; HDPE  (discontinued **)
FDA approved.Data provided by the manufacturer
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D 1238
Total Finathene® DF 210 HDPE resin  (discontinued **)
Applications: Irrigation tape and tubingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D1238
Reliance Industries Relene E41003 Polyethylene
Relene E41003 is a High Density Polyethylene grade with broad molecular weight distribution and good melt strength , suitable for making pipes for water supply, irrigation, sewage and industrial eff..
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D1238
Reliance Industries Relene L41003 Polyethylene
The UV stabilized version of Relene E41003Information provided by Reliance Industries
Melt Flow 0.28 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.28 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
SCG Chemicals EL-Leneâ„¢ H1000PBL High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stability, good resistance to weathering, good balance of MRS and SCGRecommended Applications: Water pressure pipes and stripe lines for PE100 pi..
Melt Flow 0.28 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.28 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
SCG Chemicals EL-Leneâ„¢ H1000PYL High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE100 pipe, non pressure pipesCertification: Certified by LNE..
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D 1238
Total CD 4300 HDPE extrusion
Applications: General profile extrusion, irradiation-crosslinked productsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product..
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D 1238
Total HL 428 HDPE film resin
Applications: multi-wall liner, poultry multi-layer gas flush bags, mailing envelopes, heavy-duty shipping sacks, fresh cut produce packaging, coextrusionInformation provided provided by Total Petro..
Melt Flow 0.28 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.28 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Total HL 428 HDPE Film Grade
Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro..
Melt Flow 0.28 g/10 min
0.28 g/10 min
ASTM D1238
ExxonMobil LDPE LD 358BW Low Density Polyethylene Resin (European Grade)
Product Description: LD 358BW is an EVA LDPE which offers a combination of excellent sealability and toughness even at low temperatures.Availability: Europe Additive: Antiblock: NoSlip: No Thermal ..
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D 1238
Total Finathene® HL 328 HDPE resin  (discontinued **)
Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by ..
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D 1238
Total CD 471 HDPE conduit
Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Melt Flow 0.28 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.28 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 59D HDPE Blow Molding Resin  (discontinued **)
Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer.
Melt Flow 0.28 g/10 min

@Load 2.16 kg
0.28 g/10 min

@Load 4.76 lb
ASTM D1238
Reliance Industries Relene B31101 Polyethylene
Steel pipe coating base High Density Polyethylene resin. Characteristics:broad molecular weight distribution, good melting strength, excellent toughness/ESCR, and good cut through/abrasion resistanc..