Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products GC30P200-01BG 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, General Purpose Black, Blow Molding Grade Applications: Load floorSeat backFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 0.40 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.40 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 100 Styrene Methyl Methacrylate Copolymer Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® HE-Y449-A HDPE Extrusion Resin Features: High ESCR, good toughness, good chemical resistance, good processability.Applications: Pipe coatings, profile extrusions, sheet extrusion for thermoforming, corrugated tubing, conduit.Data.. |
|||
Melt Flow | 0.40 g/10 min @Load 5.00 kg |
0.40 g/10 min @Load 11.0 lb |
ISO 1133 |
Total Lacqtene® 2001 TMA 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TMA 46 is a brown stripe compound designed to be used in combination with LACQTENE® 2001 TBK 46 for gas pipe application. The base polymer of LACQTENE® 2001 TMA 46 is the same as t.. |
|||
Melt Flow | 0.40 - 0.70 g/10 min | 0.40 - 0.70 g/10 min | |
Kazanorgsintez 102-57 Low Density Polyethylene Composite, for Further Radiation Modification Production Method: Composition is produced on the basis of 10204-003 base grade low density polyethylene or first and primary grades. Application: Used for heat and radiation resistant wires and.. |
|||
Melt Flow | 0.40 - 0.75 g/10 min | 0.40 - 0.75 g/10 min | ±18% |
Kazanorgsintez 297-285 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Melt Flow | 0.40 - 0.80 g/10 min | 0.40 - 0.80 g/10 min | ±10% |
Kazanorgsintez PE80B-285SL High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
LyondellBasell Alathon® L5040 High Density Polyethylene, Blow Molding/Extrusion Grade Alathon L5040 is able to incorporate high levels of post consumer recycle and retain excellent bottle physical properties. This resin provides high ESCR and processing stability. Typical application.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade Petrothene L3035 is a fractional melt index LDPE resin that exhibits an exceptional balance of optics, modulus, puncture, tear and shrink characteristics. Typical applications include collation shri.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
Hyosung Topilene B200 PP B200 Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:StiffnessFormabilityInformation provided by Hyosung Corporation |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 1-8000 Polypropylene Homopolymer INNOPOL® CS 1-8000 is a polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-8000 is highly suitable for manufacturing indoor waste wate.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ISO 1133 |
Iran Petrochemical (PCC) EPD 60 R Polypropylene EPD 60 R has a high molecular weight giving it superior toughness even at low temperature. It has excellent heat and detergent resistance.Applications: extrusion blow molding applications include t.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
LyondellBasell Alathon® L5040TC High Density Polyethylene ApplicationsALATHON L 5040TC is a bimodal high density polyethylene copolymer natural resin designed for telecommunications conduits. L 5040TC offers an excellent balance of stiffness, toughness and.. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Astryn BE17FC Polypropylene Copolymer, 40% Calcium Carbonate Key Features: fractional melt flow, medium high modulus, UV-stabilized, mineral-filled, blow molding and extrusion grade polypropylene copolymer, excellent impact and stiffness balance, good melt st.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ISO 1133-1981E |
LyondellBasell DP 0110M Polybutene Key Features: highly isotactic, semi-crystalline nucleated homopolymer, good creep resistance, good environmental stress crack resistance, FDA acceptable, easily dispersibleApplications: packaging i.. |
|||
Melt Flow | 0.40 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.40 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
SCG Chemicals EL-Leneâ„¢ H5211PC High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA, LNE, AENOR,.. |
|||
Melt Flow | 0.40 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.40 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorSafe™ ME3420 MDPE Compound for Pressure Pipes BorSafe™ ME3420 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an .. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 4208 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 - ISO 1133 |
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Total L425 HDPE Film Blown film polyethylene grade. Provides excellent bubble stability, exceptional tear strength, high impact and puncture resistance, outstanding clarity and gloss, good stiffness, excellent compatibi.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
UBE B028 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Melt Flow | 0.40 - 1.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.40 - 1.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 9501 Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Dow INSPIRE™ 112 Performance Polymer INSPIRE™ 112 Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion.Information provided by Dow |
|||
Melt Flow | 0.40 - 0.70 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.40 - 0.70 g/10 min @Load 11.0 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene TS High Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
Aaron Industries AAROLENE® ARPE HD 300-2 Black BM High Density Polyethylene, Blow Molding AAROLENE® ARPE 300 Series Polyethylene Compounded Resin, HDPE Black, Blow Molding GradeFeatures: A high density Polyethylene compound, pre-colored black, specifically designed for all blow molding.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
Aclo Accucomp ABS ABS809SL Extrusion Grade |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | |
Ashley Polymers Ashlene® ABS Resin F-217 General purpose super high impact with good gloss.Data provided by the manufacturer |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
UBE V106 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |