Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.40 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.40 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 100 Styrene Methyl Methacrylate Copolymer Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 0.40 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.40 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 110 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 220 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 428 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® HTR237BG BK320 TPC-ET
(Unverified Data**) Hytrel® HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal durometer hardness of 45D, is pigmented black with fine particle size carbon black an.. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
NOVA Chemicals Dylark® 378P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Melt Flow | 0.40 g/10 min @Load 5.00 kg |
0.40 g/10 min @Load 11.0 lb |
ISO 1133 |
Total Lacqtene® 2001 TYL 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TYL 46 is a cadmium-free yellow stripe compound designed to be used in combination with LACQTENE® 2001 TBK 46 for gas pipe application. The base polymer of LACQTENE® 2001 TYL 46 is.. |
|||
Melt Flow | 0.40 - 0.70 g/10 min | 0.40 - 0.70 g/10 min | |
Kazanorgsintez 102-57 Low Density Polyethylene Composite, for Further Radiation Modification Production Method: Composition is produced on the basis of 10204-003 base grade low density polyethylene or first and primary grades. Application: Used for heat and radiation resistant wires and.. |
|||
Melt Flow | 0.40 - 0.65 g/10 min | 0.40 - 0.65 g/10 min | ±10% Superior Class, ±18% 1st Class |
Kazanorgsintez 273-83 High Density Polyethylene Composite Production Method: Gaseous-phase method. Application: Composition of HD grade 273-83 is intended to obtain by method of extrusion products of industrial, cultural, and general use as well as goo.. |
|||
Melt Flow | 0.40 - 0.70 g/10 min | 0.40 - 0.70 g/10 min | ±18% |
Kazanorgsintez 293-285 High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Melt Flow | 0.40 - 0.80 g/10 min | 0.40 - 0.80 g/10 min | ±10% |
Kazanorgsintez PE80B-285D High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade Petrothene L3035 is a fractional melt index LDPE resin that exhibits an exceptional balance of optics, modulus, puncture, tear and shrink characteristics. Typical applications include collation shri.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
LyondellBasell Purell® PE3220D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding Purell PE 3220 D is a low density polyethylene with high rigidity and good chemical resistance. It is delivered in pellet form. Target markets are packaging of pharmaceuticals in the small blow mold.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
Hyosung Topilene B240LP PP B240LP Extrusion Impact CopolymerApplications:Extrusion blow moldingCharacteristics:High impactHeat stabilityInformation provided by Hyosung Corporation |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 2-8000 Polypropylene Block-Copolymer INNOPOL® CS 2-8000 is a polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8000 is highly suitable for pipe manufacturing where the required.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ISO 1133 |
Iran Petrochemical (PCC) EPD 60 R Polypropylene EPD 60 R has a high molecular weight giving it superior toughness even at low temperature. It has excellent heat and detergent resistance.Applications: extrusion blow molding applications include t.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 5401 BLK Ash is 4.71%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ISO 1133-1981E |
LyondellBasell DP 0110M Polybutene Key Features: highly isotactic, semi-crystalline nucleated homopolymer, good creep resistance, good environmental stress crack resistance, FDA acceptable, easily dispersibleApplications: packaging i.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ISO 1133 |
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SCG Chemicals EL-Leneâ„¢ H5840B High Density Polyethylene Blow Molding Key Characteristics:Excellent environmental stress cracking resistance (ESCR)Excellent appearanceOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for food, juice, sof.. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Borealis Casico™ FR4803 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing Borstar FR4803 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4803 offers a unique combination of good extrusion p.. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 - ISO 1133 |
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: .. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
Aclo Accutech ABS ABS832G30L Glass Reinforced |
|||
Melt Flow | 0.40 - 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.40 - 1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
UNI EN ISO 1133 |
Breplast Bretene LD PIPE Low Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
Aaron Industries AAROLENE® ARPE HD 300-2 Black BM High Density Polyethylene, Blow Molding AAROLENE® ARPE 300 Series Polyethylene Compounded Resin, HDPE Black, Blow Molding GradeFeatures: A high density Polyethylene compound, pre-colored black, specifically designed for all blow molding.. |
|||
Melt Flow | 0.40 g/10 min | 0.40 g/10 min | ASTM D1238 |
Aclo Accucomp ABS ABS804L High Impact Grade |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ LD 705.MJ Blown Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 705.MJ is a fractional melt index, 12.8 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and.. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polyram RamOfin PPC104 Polypropylene Copolymer Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram. |
|||
Melt Flow | 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 99C HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, excellent stretchability, high stiffness, superior strength, gel-free.Applications: Industrial woven bags, tarpaulins.Data provided by the manufacturer. |
|||
Melt Flow | 0.40 g/10 min @Load 5.00 kg |
0.40 g/10 min @Load 11.0 lb |
ISO 1133 |
Total Lacqtene® 2001 TBL 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TBL 46 is a blue stripe compound designed to be used in combination with LACQTENE® 2001 TBK 46 for gas pipe application. The base polymer of LACQTENE® 2001 TBL 46 is the same as th.. |