Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SABIC 6821N Linear Low Density Polyethylene for Blown Film Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resi.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a .. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Surpass® FPs021-F Octene sLLDPE Film Resin, 75 Micron Film FPs021-F complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |
|||
Melt Flow | 0.80 g/10 min @Load 3.80 kg, Temperature 230 °C |
0.80 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CA - 1000 E-2 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | Exxon Method |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin, 0.6 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L62608PE Film (Hexene Grade) LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |
|||
Melt Flow | 0.80 - 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Iran Petrochemical (PCC) Tabriz 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 3048 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melt Flow | 0.80 g/10 min @Load 5.00 kg, Temperature 230 °C |
0.80 g/10 min @Load 11.0 lb, Temperature 446 °F |
nozzle diam 2.095 mm; ISO 1133 |
Inno-Comp INNOPOL® CS 2-7120 20% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-7120 is a 20 % talc-filled polypropylene block-copolymer compound /PP-B TD20 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-7120 is recomme.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® LR686001 High Density Polyethylene ApplicationsPETROTHENE LR686001 is designed for use as insulation for foam/skin telephone singles, and is a natural, expandable, high density polyethylene compound containing a chemical blowing agen.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
UBE F023 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
Base Resin; ISO 1133 |
Borealis Superclean™ LE4244 Natural Crosslinkable Polyethylene for HIV Power Cable Insulation Superclean LE4244 is a natural crosslinkable polyethylene compound developed especially for the insulation of medium and high voltage cables. It provides an excellent balance of anon-staining antio.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 770 Ethylene Vinyl Acetate DuPont™ Elvax® 770 is a low BHT anti-oxidant ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications: Elvax® 770 resins can be used for the following application.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | ISO 1133 |
Total FE 8000 LDPE blown film Low density radical polyethylene made by high pressure autoclave. Advised temperature profile : 160 to 200°C.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired form.. |
|||
Melt Flow | 0.80 g/10 min | 0.80 g/10 min | ASTM D1238 |
Westlake LF2018 Hexene Linear Low Density Polyethylene Westlake LF2018 is a hexene LLDPE suitable for heavy duty films and shipping sacks. This material has increased stiffness, and can be blended with LDPE for strength property enhancements..Applicatio.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L62608 Film (Hexene Grade) LLDPE Linear Low Density Polyethylene Hexene Copolymer with High Antiblock for Film Extrusion Formolene® L62608 is a linear low density grade made using gas-phase technology. The resin is designed for he.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Borsoft™ SA233CF High Impact Polypropylene Random Heterophasic Copolymer for Blown Film Borsoft SA233CF is a very soft random heterophasic copolymer, suitable for use on conventional blown film lines with air-coolingBorsoft SA233CF is especially suitable for soft packaging, hygienic fi.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 1107X93 Linear Low Density Polyethylene Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 3201.36 Linear Low Density Polyethylene Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers NPP25-0116 Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7065 NT 7 is a fractional melt, ethylene-hexene copolymer, designe.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem F008F Homopolymer Polypropylene Description: High Melt Strength, Excellent RigidityApplications: Suggested Uses Include Strapping, Sheet Extrusion, Thermoforming, CompoundingThis resin meets the requirements for olefin polymers as.. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Breplast Bretene LD Low Density Polyethylene Recovered polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 0.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem CP 741 Blow Molding Polypropylene Description: CP 741 is a low melt flow rate heterophasic copolymer. It has broad molecular weight distribution and general purpose additive package. CP 741 presents low odor/taste transfer, high mel.. |
|||
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC SF316 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Additives- Medium slip agent, Medium antiblocking agentApplications: Agricultural & i.. |
|||
Melt Flow | 0.80 - 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.80 - 1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC SN318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati.. |