Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Nylex™ 1230 Natural Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 19C Homopolymer HDPE Film Resin Film Properties. Features: Good stiffness, good barrier, high clarity, narrow MWD.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Melt Flow | 0.95 g/10 min | 0.95 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Flex® TPO D 5302 Q Data provided by Multibase. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 12J1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity.Applications: Overwrap, lamination.Data provided by the manufacturer. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 12C01G2 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, no antiblockApplications: f.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 12C01G3 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, no slip, low antiblockApplications: .. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 12C01G4 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, high slip, medium antiblockApplicati.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 12C01G5 Clarity LLDPE Key Features: clarity LLDPE resins for film extrusion applications, excellent optical properties, easy processing, high strength, good stiffness, FDA acceptable, very high slip, medium antiblockAppl.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 16501F3 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 16501F4 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets F.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 16501F6 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets .. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Montell 16501F7 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUTENE CCO550BK PE Compound Description: LUTENE CC0550BK offer the following properties: high mechanical properties, good environmental stress cracking resistance, excellent wetherability and high speed extrusion to give a smo.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Iran Petrochemical (PCC) LL22501 Linear Low Density Polyethylene 22501 is a high stiffness LLDPE blown film grade designed for applications requiring good optical properties even at low extrusion temperature. This resin combines ease of processing with low gels a.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009F Film (Butene Grade) LLDPE Extra High Molecular Weight Hexene Copolymer Formolene® L42009F is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excellent toughness and streng.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009H Film (Butene Grade) LLDPE Butene Copolymer (Barefoot/with high AO)Applications: Higher AO package for cast and stretch filmHigher AO package for cast and stretch filmMeets all requirements of the U.S. Food and Drug Administr.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009PE Film (Butene Grade) LLDPE Linear Low Density Polyethylene Butene Copolymer for Film Extrusion Formolene® L42009PE is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excell.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L62009A Film (Hexene Grade) LLDPE Hexene Copolymer (High Antiblock)Applications: Blown film applications that don’t require slip.Blown film applications that don’t require slip.Meets all requirements of the U.S. Food and Drug Admi.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L62009E2 Film (Hexene Grade) LLDPE Hexene Copolymer (High slip and antiblock)Applications: Blown film, general purpose filmBlown film, general purpose filmMeets all requirements of the U.S. Food and Drug Administration as specified i.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis VL5580 High Density Polyethylene VL5580 is a high density polyethylene. This grade is especially designed for monofilament and cast film stretch tape production. Applications: ropes, twines , nets, monofilament applications, stra.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009A Film (Butene Grade) LLDPE Butene Copolymer (High Antiblock)Applications: Blown file for either blending or extrusionBlown file for either blending or extrusionMeets all requirements of the U.S. Food and Drug Administration a.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009B Film (Butene Grade) LLDPE Butene Copolymer (Barefoot)Applications: Blown file for either blending or extrusionBlown file for either blending or extrusionMeets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009E2 Film (Butene Grade) LLDPE Butene Copolymer (Low slip and antiblock)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyo.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L42009M Film (Butene Grade) LLDPE Butene Copolymer (High slip and antiblock)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of poly.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L62009B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Blown filmBlown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L62009X Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cross laminated filmCross laminated filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg |
0.95 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8. |
Dow DOWLEX™ NG 2085 Linear Low Density Polyethylene, Ethylene-Octene Copolymer Next Generation DOWLEX® NG 2085 resin is an ethylene-octene copolymer offering superior impact and tensile strength for down-gauged consumer liner film applications. It complies with U.S. FDA regul.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent hermetic heat sealability, easy processability, high toughness and strength.Applications: Sealant web in food packaging, vacuum packaging, barrier appl.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11J4 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent hermetic heat sealability, easy processability, high toughness and strength.Applications: Sealant web in food packaging, vacuum packaging, barrier appl.. |
|||
Melt Flow | 0.95 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.95 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 13J7 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity.Applications: Film.Data provided by the manufacturer. |