Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.4 g/10 min | 1.4 g/10 min | Cond. Q; ASTM D1238 |
Multibase Nylex™ 2185 NAT Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing.. |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Nylex™ 2185 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A; ASTM D1238 |
PolyOne Maxxam™ FR PP 600 Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A; ASTM D1238 |
PolyOne Maxxam™ FR PP H6 GF25 NHFR grey Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte.. |
|||
Melt Flow | 1.4 - 2.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.4 - 2.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 1500H (S30G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Melt Flow | 1.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM Data |
Americas Styrenics Styron® 613 Polystyrene
(discontinued **) STYRON® 613 high heat, high strength general purpose polystyrene is typically used in applications requiring a clear, tough part such as office products and magnetic media enclosures. It offers goo.. |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11U4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, easy processability.Applications: Bread bags, HDPE bottle sleeves, specialty blending.Data provided by the manufacturer. |
|||
Melt Flow | 1.4 g/10 min | 1.4 g/10 min | ASTM D1238 |
Hyosung Topilene B301 PP B301 HomopolymerApplications:Thermoforming sheetsCharacteristics:High melt tensionDimensional stabilityGood optical propertyInformation provided by Hyosung Corporation |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h.. |
|||
Melt Flow | 1.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
1.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 9076 PEI Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Melt Flow | 1.4 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.4 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Silon Tabond 2002 Adhesive Resin TABOND 2002 is ethylene-octene Plastomer / LLDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.. |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Silon Tabond 2004 Adhesive Resin TABOND 2004 is a copolymer modified with maleic anhydride functional groups.Characteristics: • Strong adhesion to aminosilane treated glass, Nylon, EVOH, PET, PBT, PC, aluminium, copper, brass .. |
|||
Melt Flow | 1.4 g/10 min | 1.4 g/10 min | ASTM D1238 |
Westlake Elevate™ EF439 4.0% Ethylene Vinyl Acetate Copolymer Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio.. |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips MarFlex® D143FK Metallocene Linear Low Density Polyethylene, Blown Film This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du.. |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Fusabond® C250 Polymer Modifier DuPont™ Fusabond® C250 is a modified ethylene vinyl acetate copolymer. Used as an adhesion promoter and coupling agent. |
|||
Melt Flow | 1.4 g/10 min | 1.4 g/10 min | ASTM D1238 |
Aclo Accutech ABS ABS833G10L Glass Reinforced |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem LD5000A LDPE Blow Molding Polyethylene LD5000A is a low-density polyethylene with good mechanical properties, good ESCR, and excellent sealing characteristics. It does not contain additives. It is used in general purpose blow molded arti.. |
|||
Melt Flow | 1.4 g/10 min | 1.4 g/10 min | |
Ashley Polymers Ashlene® ABS Resin 223 Medium impact, medium flow, matte finish. Suitable for general purpose injection molding.Data provided by the manufacturer |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CH014 Polypropylene, Homopolymer, Extrusion, Strapping COPYLENE™ CH014 is a polypropylene homopolymer resin designed for extrusion applications. Applications: Raffia/Tapes/Strapping; Geotextile & Agriculture; Nets. Equivalent to Pro-fax® HL781GInforma.. |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont™ Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 2601 is an ionomer resin available for use in blown and cast film operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applicati.. |
|||
Melt Flow | 1.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D-1238 |
Chevron Phillips EA3025 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Foam egg cartonsFoam meat traysInsulation boardBi-axially oriented sheetFeatures:Ultra-high molecular weight homopolymerHigh Vicat softening temperatureNar.. |
|||
Melt Flow | 1.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
1.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 9076 PEI (Asia Pacific) Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym.. |
|||
Melt Flow | 1.4 - 1.7 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.4 - 1.7 g/10 min @Load 11.0 lb, Temperature 392 °F |
Granulate; ISO 1133/H |
SYNTHOS Krasten® 171 General Purpose Polystyrene Very good heat resistance and mechanical strength. Examples of Application:Extrusion – biaxial-oriented sheets BOPS, XPS – lightweight insulating boards, shower enclosure panels, blends with high .. |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 11E1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness.Applications: Base resin.Data provided by the manufacturer. |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Pro-fax SV152 Polypropylene Impact Copolymer Key Features: fast crystallization shortens cycle times, excellent cold impact resistance, good stiffness and impact balance, FDA acceptableApplications: automotive blow molded partsMeets FDA requir.. |