Polymer Property : Melt Flow = 1.70 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 1.70 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.70 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-3954-70 Thermoplastic Elastomer
Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire ..
Melt Flow 1.70 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.70 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-3954-80 Thermoplastic Elastomer
Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire ..
Melt Flow 1.70 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.70 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-3954-90 Thermoplastic Elastomer
Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire ..
Melt Flow 1.70 - 135 g/10 min
1.70 - 135 g/10 min
Average value: 8.33 g/10 min Grade Count:34
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu..
Melt Flow 1.70 - 6.00 g/10 min
1.70 - 6.00 g/10 min
Average value: 3.52 g/10 min Grade Count:26
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Rotational Molding Grade". Each property range of values reported is m..