Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.0 g/10 min @Load 0.325 kg, Temperature 235 °C |
10.0 g/10 min @Load 0.716 lb, Temperature 455 °F |
ASTM D1238 |
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 2770UV Thermoplastic Elastomer Notes: General Purpose; OpaqueInformation Provided by Teknor Apex |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1662-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 10.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
10.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1665-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 125 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 257 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1900 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2123 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 10.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
10.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1855PV2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2770L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW108LE Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (700000 ppm) Uses: Film; Sheet Forms: Pellets Processing Method: Injection Molding;.. |
|||
Melt Flow | 10.0 - 30.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
10.0 - 30.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1475 Specialty Polystyrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor .. |
|||
Melt Flow | 10.0 - 25.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.0 - 25.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW2442 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene TPP2020 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 20% Filler by Weight Uses: Appliance Components; Automotive Applications; Housings Forms: Pellets Process.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1269A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1420A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2519E Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPC-CC10 Natural Copolymer Polypropylene, 10% Calcium Carbonate Filled Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPC-CC20 Natural Copolymer Polypropylene, 20% Calcium Carbonate Filled Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPC-GF15 Natural Impact Polypropylene, 15% Glass Reinforced Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPC-GF20 Natural Impact Polypropylene, 20% Glass Reinforced Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPC-T20 Copolymer Polypropylene, 20% Talc Reinforced Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPH-CC40 Natural Homopolymer Polypropylene, 40% Calcium Carbonate Filled Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPH-GF20 Natural Homopolymer Polypropylene, 20% Glass Reinforced Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW0442 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Filler/Reinforcement: Calcium Carbonate Filler Uses: Film Forms: Pelle.. |
|||
Melt Flow | 10.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
10.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU600N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2770 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene CPP2030 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Copolymer Uses: Automotive Applications; Industrial Applicati.. |