Physical Properties Metric English Comments
Melt Flow 7.0 - 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 - 13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Melt Flow 11 - 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 - 13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Polyplastic Armlen® PP MF 30-3IM Polypropylene, 30% Mineral Filled
UV resistant, impact modified, heat stabilizedInformation provided by PolyPlastic Group.
Melt Flow 10 - 13 g/10 min

@Load 2.16 kg,
Temperature 380 °C
10 - 13 g/10 min

@Load 4.76 lb,
Temperature 716 °F
6`; ASTM D1238
Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)  (discontinued **)
Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl..
Melt Flow 8.0 - 13 g/10 min
8.0 - 13 g/10 min
ASTM D1238
Kolon KOCETAL® K300LO Low Odor Acetal Resin
Low odor of formaldehyde gas. Applications: Products for low odor. Information provided by API-Kolon.
Melt Flow 10 - 13 g/10 min
10 - 13 g/10 min
ASTM D1238
Kolon KOCETAL® UR302 Toughened Grade Acetal Resin
TPU added, improved toughness. Applications: Impact resistant, flexible products. Information provided by API-Kolon
Melt Flow 10.5 - 13 g/10 min
10.5 - 13 g/10 min
ASTM D1238
Kolon KOCETAL® VT301 Anti-Static Grade Acetal Resin
Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon.
Melt Flow 10 - 13 g/10 min
10 - 13 g/10 min
ASTM D1238
Kolon KOCETAL® WR301 Wear Modified Acetal Resin
Improved weather resistant grade suitable for out door use. Applications: Weather resistant products. Information provided by API-Kolon.
Melt Flow 10 - 13 g/10 min
10 - 13 g/10 min
ASTM D1238
Kolon KOCETAL® WR301LO Wear Modified Acetal Resin
Improved weather resistance and low odor of FA. Applications: Weather resistant products at closed space. Information provided by API-Kolon.
Melt Flow 10 - 13 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 - 13 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
LTL Color Compounds ColorRxâ„¢ PC-1000RX Biocompatible Polycarbonate
A biocompatible, 10 melt grade of Polycarbonate for healthcare applications.All information provided by LTL Color Compounders, Inc.
Melt Flow 10 - 13 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 - 13 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
LTL Color Compounds ColorRxâ„¢ PC-1001A Antimicrobial Polycarbonate
A 10 melt grade of Polycarbonate containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color Compounders..
Melt Flow 10 - 13 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 - 13 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
LTL Color Compounds ColorRxâ„¢ PC-1002AF Food Grade Polycarbonate
A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc.
Melt Flow 10 - 13 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 - 13 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
LTL Color Compounds ColorRxâ„¢ PC-1002ARX Biocompatible Polycarbonate
A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc.
Melt Flow 10 - 13 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 - 13 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
LTL Color Compounds ColorRxâ„¢ PC-1005ARX Biocompatible Polycarbonate
A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Col..
Melt Flow 5.0 - 13 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 - 13 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Kraton® D1160 B (SIS) Linear Triblock Copolymer
Description: Kraton D1160 B is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from South America in the physical form identified: Kr..
Melt Flow 7.0 - 13 g/10 min

@Load 5.00 kg,
Temperature 200 °C
7.0 - 13 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Kraton® D1114 P (SIS) Linear Triblock Copolymer
Description: Kraton D1114 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 19%. It is supplied from North America in the physical form identified: ..
Melt Flow 8.0 - 13 g/10 min
8.0 - 13 g/10 min
ISO 1133
Chengdu Polyster H5550 Thermoplastic Polyether-ester Elastomer (TPEE)
Medium-low modulus molding and injection grade. Contains improved color- stable antioxidants. Good balance of low and high temperature properties. Applications requiring high original color retentio..
Melt Flow 8.0 - 13 g/10 min
8.0 - 13 g/10 min
ISO 1133
Chengdu Polyster H6555 Thermoplastic Polyether-ester Elastomer (TPEE)
Medium modulus molding and extrusion grade. Contains improved color- stable antioxidants. Good balance of modulus and toughness. Parts and components of automobile, hydraulic hose and slide of eleva..
Melt Flow 9.0 - 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 - 13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Cossa Polimeri ESTALENE EN 10 C Modified Polyolefin Blend
Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l.
Melt Flow 9.0 - 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 - 13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Cossa Polimeri ESTALENE EN 10 SC Modified Polyolefin Blend
Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l.
Melt Flow 9.0 - 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.0 - 13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Cossa Polimeri ESTALENE EN 10 SSC Modified Polyolefin Blend
Formulated for injection molding or extrusion of synthetic corksCertified according to FDA standardsInformation provided by Cossa Polimeri S.r.l.
Melt Flow 9.0 - 13 g/10 min

@Load 0.325 kg,
Temperature 190 °C
9.0 - 13 g/10 min

@Load 0.716 lb,
Temperature 374 °F
die 8/2; ISO 1133
Addcomp PRIEX® 20093 Maleic Anhydride Grafted PP homopolymer
Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fiber, wood flour, natural fibers, multilayer films, aluminum foils, or mineral filled polypr..
Melt Flow 10 - 13 g/10 min
10 - 13 g/10 min
Ashley Polymers Ashlene® 1641 Polycarbonate
A general purpose injection molding grade, natural resin, UL approved. Also available as: 1641R (with release); 1643 (with UV stabilizers); 1643R (with release and UV stabilizers).Data provided by ..
Melt Flow 9.0 - 13 g/10 min
9.0 - 13 g/10 min
Biomer P226 PHB Biodegradable Polymer
PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P..
Melt Flow 10 - 13 g/10 min
10 - 13 g/10 min
Ashley Polymers Ashlene® 1041BU Polycarbonate
A general purpose injection molding grade, in black. Also available as: 1043BU (with UV stabilizers).Data provided by the manufacturer
Melt Flow 11 - 13 g/10 min

@Load 5.00 kg,
Temperature 200 °C
11 - 13 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Granulate; ISO 1133/H
SYNTHOS Krasten® 336M High Impact Polystyrene
Easy flow grade. Processed by injection moulding of intricate and thin-walled products that enables high production output.Synthos was formerly known as Kaucuk. All information provided by Synthos.