Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.20 - 6.70 g/10 min | 2.20 - 6.70 g/10 min | Average value: 4.57 g/10 min Grade Count:6 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Melt Flow | 2.20 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-97-T0214B-55 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |