Polymer Property : Melt Flow = 2.4 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 1.8 - 2.4 g/10 min
1.8 - 2.4 g/10 min
ASTM D1238
Plaskolite Optix® CA-81 UVA UV-Absorbing Acrylic Resin
Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing..
Melt Flow 1.8 - 2.4 g/10 min
1.8 - 2.4 g/10 min
ASTM D1238
Plaskolite West Optix® CA-81 UVA UV-Absorbing Acrylic Resin
Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing..
Melt Flow 1.4 - 2.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.4 - 2.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 1500H (S30G) Propylene Homopolymer
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P..
Melt Flow 1.6 - 2.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.6 - 2.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem HE 7250 LS-L HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Melt Flow 1.6 - 2.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.6 - 2.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem LTH 0212 LLDP
IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba..