Polymer Property : Melt Flow = 20.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 3.00 - 20.0 g/10 min
3.00 - 20.0 g/10 min
Average value: 8.50 g/10 min Grade Count:4
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Melt Flow 1.00 - 20.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
1.00 - 20.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB1411 Linear Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex
Melt Flow 4.00 - 20.0 g/10 min

@Load 21.6 kg,
Temperature 200 °C
4.00 - 20.0 g/10 min

@Load 47.6 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Sinpolene MBB2185 High Impact Polystyrene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (300000 ppm) Forms: Pellets Features: General PurposeInformation Provided by Teknor Apex
Melt Flow 5.00 - 20.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.00 - 20.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBW2878 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor..
Melt Flow 5.00 - 20.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.00 - 20.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBW2888 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (700000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor..
Melt Flow 5.00 - 20.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.00 - 20.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBW3422 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (700000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor..
Melt Flow 1.10 - 20.0 g/10 min
1.10 - 20.0 g/10 min
Average value: 5.68 g/10 min Grade Count:16
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a..
Melt Flow 0.700 - 20.0 g/10 min
0.700 - 20.0 g/10 min
Average value: 2.83 g/10 min Grade Count:46
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..
Melt Flow 1.00 - 20.0 g/10 min
1.00 - 20.0 g/10 min
Average value: 10.8 g/10 min Grade Count:9
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Melt Flow 6.00 - 20.0 g/10 min
6.00 - 20.0 g/10 min
Average value: 12.1 g/10 min Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
Melt Flow 5.00 - 20.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.00 - 20.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBW011LE Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor..
Melt Flow 3.00 - 20.0 g/10 min
3.00 - 20.0 g/10 min
Average value: 9.28 g/10 min Grade Count:90
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..
Melt Flow 3.00 - 20.0 g/10 min
3.00 - 20.0 g/10 min
Average value: 12.8 g/10 min Grade Count:13
Overview of materials for Polypropylene with 10% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are ..
Melt Flow 4.00 - 20.0 g/10 min
4.00 - 20.0 g/10 min
Average value: 11.1 g/10 min Grade Count:16
Overview of materials for Polypropylene with 30% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are..