Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Nylex™ 2112 FR V0 Natural Polyamide + PP Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polyplastic TechnoTep B® 45 D Thermoplastic Elastomer, Mineral Filled High mineral filled, weather stabilityInformation provided by PolyPlastic Group. |
|||
Melt Flow | 3.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® 133 PC (Asia Pacific) Nonhalogenated. 3.5 MFR. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® TD-9055-E Hexene LMDPE Film Resin Excellent stiffness and glossApplications: Diaper back sheet, BlendingAdditives: High temperature AOFilm properties are typical of cast film extruded at 280°C.Information provided by NOVA Chemicals.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® TF-0338-E Hexene LMDPE Film Resin Excellent stiffness and glossApplications: Diaper back sheet, BlendingAdditives: High temperature AOFilm properties are typical of film extruded at 280°C.Information provided by NOVA Chemicals. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
Procedure A; ASTM D1238 |
PolyOne Elastamax™ EG-9177 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm³/10 min |
Polimeri Europa KOBLEND HI 41 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend with very good impact behaviour, ductility even at low temperatures, resistant to solvents, good dimensional stability, goo.. |
|||
Melt Flow | 3.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® 134 PC (Asia Pacific) 3.5 MFR. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not be used for medical applicati.. |
|||
Melt Flow | 3.5 g/10 min | 3.5 g/10 min | Condition G |
Ineos Nova 5800 High Impact Polystyrene
(discontinued **) Balance of toughness and rigidity, Good gloss, USP Class VIApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection .. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® TR-0338-UIG Hexene MDPE Rotational Molding Resin Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, .. |
|||
Melt Flow | 3.5 g/10 min | 3.5 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (1.5 mil Film) ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 235 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG .. |
|||
Melt Flow | 3.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
Ineos ABS Lustran® 130 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection moldingSheet extrusionBlow moldingThermoforming |
|||
Melt Flow | 3.5 g/10 min | 3.5 g/10 min | ISO 1133 |
Lucite International Diakon® TD510 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Melt Flow | 3.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution Clearblend 145 MBS Clearblend 145 is an impact modified styrene acrylic copolymer blend with excellent clarity.Excellent clarityLow densityEase of processingLow moisture absorptionInformation provided by Styrolution |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis BC545MO Polypropylene Copolymer BC545MO is a low-blush polypropylene heterophasic copolymer intended for injection molding. This grade features high impact strength, high thermal stability and very good process ability. As all pol.. |
|||
Melt Flow | 3.5 g/10 min | 3.5 g/10 min | ASTM D1238 |
UBE F320 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Total PSC 529 Polystyrene Polystyrene 529 is a medium flow crystal specially formulated for mar resistance. The easy to process crystal minimizes visual defects from ejection and automated part handling. Typical applications.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 235 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238R |
UBE UBESTA® 3030JLX2 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: semi-plasticized, UV resistance, heat resistanceInformation provided by UBE. |
|||
Melt Flow | 3.5 g/10 min | 3.5 g/10 min | Exxon Method |
ExxonMobil EXACT™ 4150 Plastomer Product Description: Exact 4150 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4150 is designed for multilayer coextruded cast film a.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Appeel® 72D727 Sealing Resin DuPont™ Appeel® 72D727 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP.. |
|||
Melt Flow | 3.5 g/10 min | 3.5 g/10 min | ASTM D1238E |
Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymer, medium slip, cast/blown film resinCharacteristics: good optics, good drawdown, can be used straight or blended with LDPE or HDPE, can b.. |
|||
Melt Flow | 3.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Dow Tyril® 880 SAN TYRIL® 880 SAN copolymer offers excellent physical properties incorporating the highest levels of chemical resistance, heat resistance and overall strength of any TYRIL grade.Data provided by Dow C.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 235 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Orgalloy® LE 60F Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).lower in viscosity than LE 6000. Suited to cast film extrusion. Inj.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 235 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 455 °F |
after drying; ISO 1133 |
Arkema Group Orgalloy® LE 60XV Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CAPILENE® TG 50 Polypropylene Impact Copolymer Description: CAPILENE® TG 50 is a heterophasic copolymer designed for injection molding applications requiring optimal impact resistance. This grade combines excellent impact strength, even at lo.. |
|||
Melt Flow | 3.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min. |
Ineos ABS Lustran® 452
(discontinued **) Key Features:UnfilledSuitable processing methods:Sheet extrusionThermoformingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after I.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem H 501 HC Bioriented Film Polypropylene Applications: High stiffness; barrier films for conversionInformation provided by Braskem |