Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 260 °C |
33 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C4210HF is a 10% glass reinforced, non-FR PC+ABS grade with high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low sh.. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 200 °C |
33 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 200 °C |
33 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 330 °C |
33 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 330 °C |
33 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 330 °C |
33 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 330 °C |
33 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Europe-Africa-Middle East) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® HD-6733 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: High Flow, Good StiffnessUses: Food containers, Small pails, Nursery containers |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 220 °C |
33 g/10 min @Load 22.0 lb, Temperature 428 °F |
Estimated using room temperature density |
Ineos ABS Lustran® M203FC Standard impact strength, easy flowing, high gloss, BgVV and FDA quality for food contact. ,Property data per ISO test methods. |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 220 °C |
33 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical SG175 ABS, Super Surface Gloss Feature: Injection Molding, Super Surface GlossApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 200 °C |
33 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Kraton® D4158 K (O/E SBS) Radial Copolymer Description: Kraton D4158 K is an oiled, radial copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form: Kraton D4158 KT - .. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 260 °C |
33 g/10 min @Load 4.76 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Pocan® B 3215 901510 PBT, 10% Glass Fiber PBT, 10% glass fibers, injection molding |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 266 °C |
33 g/10 min @Load 2.65 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 266 °C |
33 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V8280 PBT+PET 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 250 °C |
33 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HN-3102G PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 220 °C |
33 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® BF-0930 MABS, Unreinforced Scratch Resistant Scratch resistantInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 220 °C |
33 g/10 min @Load 22.0 lb, Temperature 428 °F |
|
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 220 °C |
33 g/10 min @Load 22.0 lb, Temperature 428 °F |
|
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 250 °C |
33 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX2790C PPE+HIPS (Asia Pacific) PPE/HIPS unfilled FR-V1, 90C |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 266 °C |
33 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V8280 PBT+PET (Europe-Africa-Middle East) 40% GR PBT+PET. High stiffness. Excellent surface aesthetics. Applications include office furniture. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE HD 6733.17 High Density Polyethylene Copolymer Resin Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable .. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 250 °C |
33 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection .. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LD 506.07 Compounding and molding resin Product Description: LD 506.07 is a high flow, LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.Availabilit.. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 506.07 Low Density Polyethylene Resin Product Description: LD 506.07 is a high flow, LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.Availabilit.. |
|||
Melt Flow | 33 g/10 min | 33 g/10 min | ISO 1133 |
Domo 1040SC Polypropylene Homopolymer Information provided by Domo. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 230 °C |
33 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CAPILENE® HU 75 AV Polypropylene Impact Copolymer Description: CAPILENE® HU 75 AV is a nucleated and antistatic controlled rheology impact copolymer for injection molding. It is characterized by improved stiffness and medium impact resistance. .. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 250 °C |
33 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 220 °C |
33 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali |