Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CP - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers NPP 808 C3WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 4.5 - 7.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.5 - 7.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 1500L (C30G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Melt Flow | 4.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
4.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
Internal Method |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers 707 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM 1238G |
Total Lacqrene® 3351(AS) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
DIN 5375/ISO 1133 |
Ineos Nova S-6600 High Impact Compact Polystyrene
(discontinued **) High impact polystyrene which is very easy processed in extension and thermoforming processes. Typical applications are packaging of food stuffs like Yot beakers but technical parts and extruded pr.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LE-0520-A LDPE Extrusion Resin
(discontinued **) Features: easy processing, good dispersion.Applications: Additive and color concentrates for film and molding.Data provided by the manufacturer. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade ALATHON M5352 is a high density copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good proces.. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238 |
LyondellBasell Plexar® PX3243 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, s.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 1-4140 BAP 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-4140 B AP is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-4140 B AP is recommended especially for producing products, where high stif.. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238 |
KKPC Kuhmo HI 425 E Extrusion Molding HIPS Key features: Cold-resistant Extrusion. Common Uses: Refrigerator inner liners, door liners, disposable cups, food packaging sheet, wrapping films, trays, washing machinesHIPS is a functional resin .. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238G |
Hannam Chemical Hanalac 750 ABS, General Purpose FDA Approved. Good combination of impact strength, rigidity, gloss, heat resistance, processability, and thermal stability. May be injection molded. Its broad range of applications include: elect.. |
|||
Melt Flow | 4.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
TPI Porene® KU900 Super High Heat ABS INJECTION MOLDING. ELECTRICAL PARTS, AUTOMOTIVE APPLICATIONS, HOUSEHOLD GOODS, TOYSPorene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymer.. |
|||
Melt Flow | 4.5 - 7.5 g/10 min @Temperature 230 °C |
4.5 - 7.5 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 4.5 - 7.5 g/10 min | 4.5 - 7.5 g/10 min | Cond L; ASTM D1238 |
Washington Penn PPUP4G402 Polypropylene, 40% Talc Filled, High Flow Exceptional retention of mechanical properties and appearance upon long term heat aging.Applications: Appliance parts.Data provided by Washington Penn Plastic Co., Inc. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Total EVA 1040 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1040 VN 4 is made by a high pressure tubular process. Grade for very flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Thin st.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133H |
Total PSI 8350 High Impact Polystyrene 8350 is a very high impact polystyrene for extrusion. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. It is proposed for the produc.. |
|||
Melt Flow | 4.5 - 7.5 g/10 min @Temperature 230 °C |
4.5 - 7.5 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis CA7230 Low Density Polyethylene CA7230 is a low-density polyethylene for extrusion coating. CA7230 contains no additives. Applications: Extrusion coating of high volume production of boards and papers. Coating of various plasti.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Xmod™ GD301FE Polypropylene, Glass Fiber Reinforced Xmod™ GD301FE is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also a.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Exceed™ 4518PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 4581PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 4581PA have outstanding tensile properties and impact and puncture toughness. These superior prope.. |
|||
Melt Flow | 4.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
4.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GM7746CA HDPE Blow Molding Polyethylene GM7746CA is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tena.. |
|||
Melt Flow | 4.5 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
die 8/2; ISO 1133 |
Addcomp PRIEX® 15005 Maleic Anhydride modified LDPE Functionalised low density polyethylene to be used as compatibiliser for polymer blends or coupling agent for wood flour, natural fibres, or mineral filled polyolefins. Also suitable to reduce pigme.. |
|||
Melt Flow | 4.5 - 7.5 g/10 min @Load 1.05 kg, Temperature 400 °C |
4.5 - 7.5 g/10 min @Load 2.31 lb, Temperature 752 °F |
ASTM D1238 |
Mitsui AURUM® PL450C Polyimide
(discontinued **) AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU.. |
|||
Melt Flow | 4.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min |
Polimeri Europa SINKRAL PD C823 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-35-15 Injection moulding grade, exhibiting very high impact resistance, even at low temperatures. Applic.. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Luriblend® ABS TL10 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 230 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Arkema Group Kynar® 4000 HD PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1N,Q.?E5.I.B.E.C,, ?(6-10)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high b.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Nova Zyntar® 707 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |