Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SABIC PP 6711K Polypropylene Copolymer for Injection Molding Product Description: PP 6711K is a controlled rheology grade with narrow molecular weight distribution intended specifically for producing injection molded articles with high clarity, good flow pro.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 190 °C |
45 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Total Finaprene® 411x Styrene-Butadiene TPE Copolymer Compounded to 59 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 411x is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its high molecular weight, Finaprene® 411x provides e.. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | ASTM D1238 |
Hyosung Topilene J842 PP J842 Injection Impact CopolymerApplications: Very large articles:Washing M/C partsIndustrial applianceCharacteristics:High flowabilityHigh stiffnessInformation provided by Hyosung Corporation |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
L; ASTM D1238 |
Global PP-1140-T Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-disposable drinkware, thin-walled partsInformation provided by Global Polymers Corporation. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 200 °C |
45 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kraton® D1162 P (SIS) Linear Triblock Copolymer Description: Kraton D1162 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 43%. It is supplied from North America in the physical form identified: .. |
|||
Melt Flow | 45 g/10 min @Load 10.0 kg, Temperature 380 °C |
45 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1502-7865/BK2 PPSU, unreinforced Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 270 °C |
45 g/10 min @Load 11.0 lb, Temperature 518 °F |
ISO 1133-1 |
Lanxess Pocan® C 1202 000000 PET + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | ISO 1133-1981E |
LyondellBasell DP 8510M Polybutene Key Features: semi-crystalline high ethylene content random copolymer, miscible with polyproylenesApplications: Hot Melt Adhesives, FDA acceptableMeets FDA requirements in 21 CFR 175.105 for indirec.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 316 °C |
45 g/10 min @Load 11.0 lb, Temperature 601 °F |
Procedure B; ASTM D1238 |
Solvay Specialty Polymers Ryton® QC160N Polyphenylene Sulfide (PPS) Ryton® QC160N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Ch.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 316 °C |
45 g/10 min @Load 11.0 lb, Temperature 601 °F |
Procedure B; ASTM D1238 |
Solvay Specialty Polymers Ryton® QC160P Polyphenylene Sulfide (PPS) Ryton® QC160P (pelletized) polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and is suitable for thermoplastic extrusion processes.Features: Good Chemical Resista.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 260 °C |
45 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/ASA FR1508 UV Availability: North AmericaForms: PelletsAdditive: Flame Retardant and UV StabilizerFeatures: Flame Retardant, Good UV Resistance and Halogen FreeInformation provided by TP Composites, Inc. |
|||
Melt Flow | >= 45 g/10 min @Load 10.0 kg, Temperature 220 °C |
>= 45 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Absolan® 2150 SAN Absolac 2150 Crystal is a heat and chemical resistant gradeInformation provided by Styrolution |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 280 °C |
45 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis BH374MO Polypropylene Copolymer BH374MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. Products molded with this grade exhibi.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis BH980MO Polypropylene Copolymer BH980MO is a heterophasic copolymer. This grade provides very high stiffness, high gloss and low stress whitening. and is designed for high-speed injection molding and contains nucleating and antist.. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | ASTM D1238 |
Total PPH 3847MR Polypropylene, Radiation Resistant - Clarified - High Flow for Injection Molding TOTAL Petrochemicals Polypropylene 3847MR offers good processability, excellent clarity, good toughness and good resistance to typical levels of gamma radiation used to sterilize polypropylene.Easy .. |
|||
Melt Flow | 45 - 65 g/10 min @Load 8.70 kg, Temperature 190 °C |
45 - 65 g/10 min @Load 19.2 lb, Temperature 374 °F |
|
Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane Feature: Excellent flame retardant properties, matt surface appearance and low surface friction and transparent spherical pelletsUses: Melt roll coated fabrics and calenderingAvailable in Americas, .. |
|||
Melt Flow | 45 g/10 min @Load 10.0 kg, Temperature 220 °C |
45 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
Cossa Polimeri ESTADIENE 1218 V0/B Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 330 °C |
45 g/10 min @Load 4.76 lb, Temperature 626 °F |
ISO 1133 |
Covestro Apec® 1695 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=158 °CPreprocessingMax. Water content |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 260 °C |
45 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Covestro Makroblend® DP UT3907 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT3907* offers superior flowability, good impact strength and excellent ch.. |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | ASTM D1238 |
ExxonMobil Escorene™ UL 04533EH2 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 04533EH2 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Fre.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 230 °C |
45 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TI4450M Impact Copolymer Polypropylene Description: Very High Flexural ModulusApplications: Suggested Uses Include Compounding, Automotive Interior Trim, Intricately Designed Parts, Thin-Walled Parts.Process: Compounding.This resin meets.. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 190 °C |
45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Barlog Plastics KEBAFORM C 520.0 POM Copolymer unreinforced POMInformation provided by BARLOG plastics GmbH. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 190 °C |
45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Beijing Ranger Chem BLUESTAR® BS450 Acetal Copolymer Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Flow | 45 g/10 min @Load 10.0 kg, Temperature 220 °C |
45 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-17 A EP ABS Electro Plating Applications Electroplating & Hot Stamping GradesInformation provided by Bhansali |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 190 °C |
45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem IJ33D LLDPE Injection Molding Polyethylene Copolymer IJ33D is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, excellent flexibi.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 275 °C |
45 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 GF35 Polyamide 6 - Glass Fiber Reinforced 35% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Melt Flow | 45 g/10 min @Load 10.0 kg, Temperature 220 °C |
45 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-17 A EP ABS Electro Plating Applications Electroplating & Hot Stamping GradesInformation provided by Bhansali |
|||
Melt Flow | 45 g/10 min | 45 g/10 min | (MVR) [cm³/10min]; ISO 1133 |
EMS-Grivory Grivory® F 50 nat 6368 PA6 Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro.. |