Polymer Property : Melt Flow = 6.8 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escorene® LL-8555 LLDPE, Rotational Molding Pellets  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escorene® LL-8556 LLDPE, Rotational Molding Powder  (discontinued **)
Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Formosa Plastics Formolene® L63568 Rotational Molding LLDPE  (discontinued **)
Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568 is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. The..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Formosa Plastics Formolene® L63568U Rotational Molding LLDPE  (discontinued **)
Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. Th..
Melt Flow 6.8 g/10 min
6.8 g/10 min
ExxonMobil Method
ExxonMobil LD 102.74 Thin Gauged Film Resin  (discontinued **)
LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical
Melt Flow 6.8 g/10 min
6.8 g/10 min
ASTM D1238
LyondellBasell Alathon® M5370PX High Density Polyethylene, Extrusion Grade
ALATHON M5370PX is a copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processability. T..
Melt Flow 6.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
LG Chemical 15NFE GPPS
High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio..
Melt Flow 6.8 g/10 min

@Load 6.60 kg,
Temperature 337 °C
6.8 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM CRS5711 PEI
15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing.
Melt Flow 6.8 g/10 min

@Load 6.60 kg,
Temperature 337 °C
6.8 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM CRS5711 PEI (Asia Pacific)
15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing.
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Total PPR 8573 Polypropylene, Film Extrusion Grade
Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8573 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The low m..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LD 102.LC Thin Gauged Film Resin
L Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawndown to thing gauges.Availability: Latin America, North America and ..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LDPE LD 102.LC Low Density Polyethylene Resin
Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawn down to thing gauges.Availability: Latin America, North America and S..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LL 6407.67 Injection Molding Resin
L Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processa..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LL 8555.24 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LL 8555.25 Rotational Molding Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LLDPE LL 6407.67 Linear Low Density Polyethylene Resin
Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processabi..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Fainplast Compounds Ethylplus 613 HPE Polyethylene Cable Compound
Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesExpandable HDPE by gas injectionInformation provided ..
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
BASF Ultraform® N2640 E2 POM
Description: Is a POM + MBS, elastomer-modified injection-molding grade with enhanced toughness and high weld line strength.Information provided by BASF
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Braskem CP 405 XP Injection Molding Polypropylene
Applications: Caps for soft drinks. Information provided by Braskem
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Braskem CP 405XP Compression Molding Polypropylene Heterophasic Copolymer
Bottle caps for carbonated beverages.Information provided by Braskem.
Melt Flow 6.8 g/10 min
6.8 g/10 min
ASTM D1238
ExxonMobil LL 8555.67 Rotational Molding Resin  (discontinued **)
LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir..
Melt Flow 6.8 g/10 min
6.8 g/10 min
DuPont Fusabond® MB528D Linear Low Density Polyethylene  (discontinued **)
Typical Use: Coupling agent for filled PE systems such as nonhalogen flame retardant filled wire and cable compoundsAdhesion promoterAvailability: North AmericaInformation provided by DuPont.
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LL 6407 Injection Molding Resin  (discontinued **)
LL 6100 is a narrow molecular weight butene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processability with minimal wa..
Melt Flow 6.8 g/10 min
6.8 g/10 min
Exxon Method
ExxonMobil Escorene® LL-8556 LMDPE Rotational Molding Grade  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene having improved flow characteristics vs. LL-8300's series resins, yet retaining outstanding whiteness and a goo..