Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® LL-8555 LLDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® LL-8556 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L63568 Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568 is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. The.. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® L63568U Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. Th.. |
|||
Melt Flow | 6.8 g/10 min | 6.8 g/10 min | ExxonMobil Method |
ExxonMobil LD 102.74 Thin Gauged Film Resin
(discontinued **) LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical |
|||
Melt Flow | 6.8 g/10 min | 6.8 g/10 min | ASTM D1238 |
LyondellBasell Alathon® M5370PX High Density Polyethylene, Extrusion Grade ALATHON M5370PX is a copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processability. T.. |
|||
Melt Flow | 6.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
6.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical 15NFE GPPS High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio.. |
|||
Melt Flow | 6.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
6.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5711 PEI 15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 6.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
6.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5711 PEI (Asia Pacific) 15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Total PPR 8573 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8573 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The low m.. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LD 102.LC Thin Gauged Film Resin L Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawndown to thing gauges.Availability: Latin America, North America and .. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 102.LC Low Density Polyethylene Resin Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawn down to thing gauges.Availability: Latin America, North America and S.. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LL 6407.67 Injection Molding Resin L Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processa.. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LL 8555.24 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LL 8555.25 Rotational Molding Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 6407.67 Linear Low Density Polyethylene Resin Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processabi.. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LLP 8555.24 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Fainplast Compounds Ethylplus 613 HPE Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesExpandable HDPE by gas injectionInformation provided .. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® N2640 E2 POM Description: Is a POM + MBS, elastomer-modified injection-molding grade with enhanced toughness and high weld line strength.Information provided by BASF |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238L |
Braskem CP 405 XP Injection Molding Polypropylene Applications: Caps for soft drinks. Information provided by Braskem |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem CP 405XP Compression Molding Polypropylene Heterophasic Copolymer Bottle caps for carbonated beverages.Information provided by Braskem. |
|||
Melt Flow | 6.8 g/10 min | 6.8 g/10 min | ASTM D1238 |
ExxonMobil LL 8555.67 Rotational Molding Resin
(discontinued **) LL 8555 is a linear low density hexene copolymer designed to offer excellent processability, dimensional control, whiteness and low warpage. This resin is ideally suited for applications that requir.. |
|||
Melt Flow | 6.8 g/10 min | 6.8 g/10 min | |
DuPont Fusabond® MB528D Linear Low Density Polyethylene
(discontinued **) Typical Use: Coupling agent for filled PE systems such as nonhalogen flame retardant filled wire and cable compoundsAdhesion promoterAvailability: North AmericaInformation provided by DuPont. |
|||
Melt Flow | 6.8 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.8 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LL 6407 Injection Molding Resin
(discontinued **) LL 6100 is a narrow molecular weight butene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processability with minimal wa.. |
|||
Melt Flow | 6.8 g/10 min | 6.8 g/10 min | Exxon Method |
ExxonMobil Escorene® LL-8556 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene having improved flow characteristics vs. LL-8300's series resins, yet retaining outstanding whiteness and a goo.. |