Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.0 - 8.9 g/10 min | 5.0 - 8.9 g/10 min | ASTM D1238 |
Shuman 502 Black Polypropylene Copolymer Good impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer. |
|||
Melt Flow | 5.0 - 8.9 g/10 min | 5.0 - 8.9 g/10 min | ASTM D1238 |
Shuman 502C Black Polypropylene Copolymer Excellent impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer. |
|||
Melt Flow | 5.0 - 8.9 g/10 min | 5.0 - 8.9 g/10 min | ASTM D1238 |
Shuman 510 Black Polypropylene Homopolymer Excellent chemical resistance, excellent processabilityData provided by the manufacturer. |