Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 10.0 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 254 microns
10.0 mil
Parker Chomerics Tecknit® 0035 Conductive Silicone Sealant/Adhesive
Comments: Thin flexible pasteTypical Applications: Bonding elastomer gasketInformation provided by Chomerics
Thickness 254 microns
10.0 mil
Parker Chomerics Tecknit® 0036 Two Part Flexible Adhesive-Sealant Silver-Glass Silicone
Description: TECKNIT 0036 is an electrically conductive, medium viscosity, RTV silicone adhesive-sealant. This silver-plated glass filled system is formulated with a special conductive material pro..
Thickness 254 microns
10.0 mil
Parker Chomerics Tecknit® 0192/0193 Conductive Silicone Sealant/Adhesive
Comments: Rec. bond line thickness: < 0.4 mm; flexible past.Typical Applications: Bonding Ag/Cu elastomer gaskets; thin bond gap.Information provided by Chomerics
Thickness 254 microns
10.0 mil
Hexcel® HexForce™ KA060 Aramid and High Performance Fabrics
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..
Thickness 254 microns
10.0 mil
Thickness of film tested; ASTM D374
Eastman Tritan FX200 Copolyester
Eastman Tritan FX200 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w..
Thickness 254 microns
10.0 mil
Nominal
DuPont™ Nomex® 410 Paper, 10 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Thickness 254 microns
10.0 mil
Nominal
DuPont™ Nomex® 411 Paper, 10 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..
Thickness 254 microns
10.0 mil
Nominal
DuPont™ Nomex® 414 Paper, 10 mil Nominal Thickness
Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand..
Thickness 254 microns
10.0 mil
Nominal
DuPont™ Nomex® N196 Paper, 10 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Thickness 254 microns
10.0 mil
Backing; ASTM D3652
3M 2552/Silver Damping Foils
General purpose vibration dampingInformation provided by 3M
Thickness 254 microns
10.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 19563R032 0.032" Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Cured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the producti..
Thickness 254 microns
10.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 55572XD028 0.028" (0.711 mm) Cured Silicone Rubber
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data Represents typical values for the production material. The data should not be used to write, or in place of..
Thickness 254 microns
10.0 mil
Rubber; Arlon SQA-TMS-003
Arlon 99202R010 0.010" Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction:Interleave: 0.0015" PolyethyleneSide 1: Cured Silicone RubberCarrier: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and should no..
Thickness 254 microns
10.0 mil
Side 1
Arlon 99790N010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Side 1: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used to write,..
Thickness 254 microns
10.0 mil
Side 2; Arlon SQA-TMS-003
Arlon R30711R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: PolyethyleneAppearance: Red silicone gum ..
Thickness 254 - 305 microns
10.0 - 12.0 mil
Overall
Arlon R31901R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
Thickness 254 microns
10.0 mil
3M Scotchkote™ 162CR Epoxy Coating
3M Scotchkote Epoxy Coating 162CR has been specifically developed as a 100% solids lining for eth internals of tanks, vessels and other equipment in contact with dirty water, mild aqueous chemicals ..
Thickness 254 microns
10.0 mil
3M Scotchkote™ CR 511 Epoxy Ceramic Surface
Scotchkote Epoxy Ceramic CR 511 has been specifically developed as a 100% solids coating for resurfacing and lining to improve the efficiency of equipment in fluid flow environments.Product Features..
Thickness 254 microns
10.0 mil
3M Scotchkote™ FG 512 Epoxy Ceramic Surfacer
Scotchkote Epoxy Ceramic Surfacer FG 512 has been specifically developed as a ceramic enhanced epoxy repair coating for resurfacing and reforming metal machinery and equipment, such as pumps, impell..
Thickness >= 254 microns
>= 10.0 mil
Side 2
Arlon 44566R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w..
Thickness 254 - 305 microns
10.0 - 12.0 mil
Overall
Arlon 44571B010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place..
Thickness 254 microns
10.0 mil
Side 2
Arlon 51426R020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the pr..
Thickness 254 microns
10.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 55108R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone RubberSide 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data rep..
Thickness 254 microns
10.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 55572R028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T..
Thickness 254 - 292 microns
10.0 - 11.5 mil
Side 2, Skim Coat + Uncured
Arlon R33216R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl..
Thickness 254 - 356 microns
10.0 - 14.0 mil
3M 963-10 Flexible Prismatic Conspicuity Markings
3M Flexible Prismatic Conspicuity Markings Series 963 are highly retroreflective flexible microprismatic markings designed to mark the sides and rear of vehicles for enhanced visibility and detectio..
Thickness 254 microns
10.0 mil
Side 2; Arlon SQA-TMS-003
Arlon 44141R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent..
Thickness 254 microns
10.0 mil
Overall Thickness
Arlon 44426R010 0.010" Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Cured Silicone RubberSide 2: Uncured Silicone RubberSubstrate: Prime Coated 1165 FiberglassThis data represents typical values for the p..
Thickness 254 microns
10.0 mil
Hexcel® HexForce™ 5354 Aramid Fabric
Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid..
Copyright © lookpolymers.com All Rights Reserved