Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 12.7 - 76.0 microns | 0.500 - 2.99 mil | Recommended range for processing |
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins FPs117-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Thickness | 12.7 microns | 0.500 mil | Adhesive |
Dielectric Polymers NT-5000 Protective Film
(discontinued **) Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA.. |
|||
Thickness | 12.7 - 10000 microns | 0.500 - 394 mil | Average value: 1440 microns Grade Count:15 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Thickness | 12.7 - 25400 microns | 0.500 - 1000 mil | Average value: 316 microns Grade Count:504 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Thickness | 12.7 microns | 0.500 mil | 4:1 BUR; Neck Height = 8 Die Diameters |
LyondellBasell Alathon® L4903 High Density Polyethylene ApplicationsALATHON L 4903 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits excellent machine direction tear in an HMW-HD resi.. |
|||
Thickness | 12.7 microns | 0.500 mil | |
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film Transparent, Medium Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resista.. |
|||
Thickness | 12.7 microns | 0.500 mil | |
ExxonMobil Label-Lyte® 612 LLG-102 Clear OPP Film Clear, polypropylene films designed for use in roll-fed labeling applications. This film can be laminated to itself or applied as an outer web to other films. The print surface is a treated high ene.. |
|||
Thickness | 12.7 microns | 0.500 mil | Side 1, Skim Coat |
Arlon 55578XC028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 9740 Double Coated Tape 3M™ Double Coated Tape 9740 is a 3.5 mil double coated tape utilizing a 0.5 mil (12 microns) polyester film coated on both sides with 1.5 mils (38 microns) of a high shear acrylic adhesive system. .. |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 9741R Double Coated Tape 3M™ Double Coated Tape 9741 is a 6.5 mil double coated tape utilizing a 0.5 mil hand-tearable polyester film heavily coated on both sides with 3 mils of an ultra high peel acrylic adhesive system. .. |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 9832 Double Coated Tapes with Adhesive 300MP 3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape.. |
|||
Thickness | 12.7 microns | 0.500 mil | Side 1, Skim Coat |
Arlon 55978X030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Cured/Uncured Layers Appearance: Gray silicone gum on glass fiber fabricThis data Represents typical values for the production material.. |
|||
Thickness | 12.7 microns | 0.500 mil | Side 1 |
Arlon R33073X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: 7628 FiberglassSide 2: Cured Silicone RubberInterleave: NoneThis data represents typical values for the production material and should .. |
|||
Thickness | 12.7 microns | 0.500 mil | Facestock |
3M FM002 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 12.7 microns | 0.500 mil | Side 2 |
Arlon 51163X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone Rubber50" wideThis data represents typical values for the production material and should not.. |
|||
Thickness | <= 12.7 microns | <= 0.500 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51808R011 0.011" (0.279 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat This data represents typical values for the production .. |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 9039 Double Coated Tapes with Adhesive 300 3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides.. |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 93010LE High Strength Double Coated Tape with Adhesive 300LSE 3M ™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryl.. |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 9475LEB High Strength Double Coated Tape with Adhesive 300LSE 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryli.. |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 9628FL Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 9741 Double Coated Tape 3M™ Double Coated Tape 9741 is a 6.5 mil double coated tape utilizing a 0.5 mil hand-tearable polyester film heavily coated on both sides with 3 mils of an ultra high peel acrylic adhesive system. .. |
|||
Thickness | 12.7 microns | 0.500 mil | Facestock |
3M FM001 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 9593 Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 9629B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 9629PC Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 9737R Double Coated Splicing Tape 3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres.. |
|||
Thickness | 12.7 microns | 0.500 mil | Carrier |
3M 9828 Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Thickness | 12.7 microns | 0.500 mil | |
ExxonMobil Escorene® HD-7756 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7756 exhibit excellent impact and toughness properties as well as high stiffness... |
|||
Thickness | 12.7 microns | 0.500 mil | |
ExxonMobil Label-Lyte® 612 LL-112 Clear OPP Overlaminate Clear, polypropylene film designed to provide exceptional clarity and print protection when used as an overlaminate in pressure-sensitive labeling applications. The treated high energy layer provide.. |
|||
Thickness | 12.7 microns | 0.500 mil | |
Formosa Plastics Formolene® E924F Film HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin for Film Applications Formolene® E924F is a “low gel” high molecular weight grade of HDPE designed for high dart impact strength and.. |