Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | >= 152 microns | >= 6.00 mil | Side 2 |
Arlon 518581R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th.. |
|||
Thickness | 152 microns | 6.00 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 18609R023 0.023" (0.584 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: PolyethyleneLayer 1: Cured Silicone RubberLayer 2: Uncured Silicone RubberSubstrate: 11523 Style FiberglassThis data represents typical values for the production mate.. |
|||
Thickness | 152 microns | 6.00 mil | Side 1 |
Arlon 19576R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat.. |
|||
Thickness | 152 microns | 6.00 mil | Tape Caliper |
3M 9443NP Double Coated Tapes with Adhesive 700 Series 3M™ Double Coated Tapes with 3M™ Adhesive 700 Series feature a high tack synthetic rubber adhesive which provides excellent quick stick or initial adhesion and bonds together a wide variety of mat.. |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55578R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Appearance:.. |
|||
Thickness | >= 152 microns | >= 6.00 mil | Side 1, Uncured Rubber Layer |
Arlon 55579R028M 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 56106R026 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sil.. |
|||
Thickness | 152 microns | 6.00 mil | side 1; Arlon SQA-TMS-003 |
Arlon 56276R026 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
Thickness | 152 microns | 6.00 mil | side 2; Arlon SQA-TMS-003 |
Arlon 56976R026 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber |
|||
Thickness | 152 microns | 6.00 mil | side 1; Arlon SQA-TMS-003 |
Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber |
|||
Thickness | 152 microns | 6.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 56986XA028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp.. |
|||
Thickness | 152 microns | 6.00 mil | Release Liner |
3M ATG 928 Tape 0.002 in. (0.05 mm) thick high-tack/low-tack double coated tapeInformation provided by 3M |
|||
Thickness | 152 microns | 6.00 mil | ASTM D3652 |
3M Scotch® 8915 Filament Tape Scotch® Filament Tape 8915 is a high-performance transparent tape reinforced with continuous high strength glass filaments which is designed to hold appliance parts together during manufacture and .. |
|||
Thickness | 152 microns | 6.00 mil | ASTM D3652 |
3M Scotch® 893 Filament Tape Scotch® Tape 893 is a general-purpose packaging tape reinforced with continuous glass-yarn filaments that give the tape high tensile strength and low stretch. The clear 3M™ Scotchpro™ backing pro.. |
|||
Thickness | 152 microns | 6.00 mil | Tape |
3M 410M Double Coated Paper Tapes 3M™ Double Coated Paper Tapes 401M and 410M utilize a natural rubber adhesive system that offers good to excellent adhesion to many types of surfacesInformation provided by 3M |
|||
Thickness | 152 microns | 6.00 mil | Side 1 |
Arlon 44566R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w.. |
|||
Thickness | 152 microns | 6.00 mil | side 2 silicone; Arlon SQA-TMS-003 |
Arlon 51141R020 Silicone Rubber/Fiberglass Laminate Interleave 1: 3 mil PE; Side 1: uncured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave 2: 3 mil PE |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51231R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 152 microns | 6.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51231R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 152 microns | 6.00 mil | Side 2 |
Arlon 51581R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the.. |
|||
Thickness | 152 microns | 6.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51991A020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typica.. |
|||
Thickness | 152 microns | 6.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55276R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Thickness | 152 microns | 6.00 mil | Layer 1; Arlon SQA-TMS-003 |
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Thickness | 152 microns | 6.00 mil | side 2; Arlon SQA-TMS-003 |
Arlon 56946C026 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 56986R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp.. |
|||
Thickness | 152 microns | 6.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 56986R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp.. |
|||
Thickness | >= 152 microns | >= 6.00 mil | Side 2 |
Arlon R33099G028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl.. |
|||
Thickness | >= 152 microns | >= 6.00 mil | Side 1, Uncured |
Arlon R34369R028 0.029" (0.737 mm) Uncured Layer on Top of a Cured Layer on One Side with Fiberglass Substrate, 38" wide Design/Construction:Side 1: Uncured Layer on Top of a Cured Layer on One SideThis data Represents typical values for the production material. The data should not be used to write, or in place of, ma.. |
|||
Thickness | 152 microns | 6.00 mil | ASTM D3652 |
3M Scotch® 897 Filament Tape Scotch® Tape 897 is a glass-filament-reinforced tape suitable for light to medium duty strapping, bundling, reinforced applications. Scotch® Tape 897 has a synthetic rubber resin adhesive with goo.. |
|||
Thickness | <= 152 microns | <= 6.00 mil | |
3M Scotchkote™ HG 519 Epoxy Ceramic HD Surfacer Scotchkote Epoxy Ceramic HD Surfacer HG 519 has been specifically developed as a 100% solids ceramic repair system for resurfacing equipment subject to severe abrasion.Product Features:Combines good.. |