Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 33.0 microns | 1.30 mil | Adhesive |
Dielectric Polymers NT-711 Electrical/Mechanical Tape
(discontinued **) High temperature acrylic adhesive with polyester film backing.Features: High temperature shear propertiesSolvent resistantTemperature class: 266°FInsulation resistance: > 1x106 M?Electrolytic corro.. |
|||
Thickness | 33.0 microns | 1.30 mil | |
Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film
(discontinued **) Description: ACLAR® CX 130E is a heat sealable PCTFE film with outstanding clarity. It is used where applications require moisture protection.Information provided by Honeywell. |
|||
Thickness | 33.0 microns | 1.30 mil | |
Westlake EB171 MDPE Medium Density Polyethylene Westlake EF171 is a MDPE resin suggested for use in shrink packaging applications. This material has good TD shrinkage, good optical properties, excellent machinability, and toughness. This resin gr.. |
|||
Thickness | 33.0 microns | 1.30 mil | Thickness Tested |
Westlake EF522 12% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF522 is an ethylene vinyl acetate copolymer with 12% VA. EF522 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength m.. |
|||
Thickness | 33.0 microns | 1.30 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 125 BSR-ONE OPP Film Product Description: Bicor BSR-ONE is a two-side sealable, one side treated, coextruded OPP film designed for unsupported plain or surface print applications, and in laminations on both HFFS and VF.. |
|||
Thickness | 33.0 microns | 1.30 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 220 AB OPP Film Product Description: Bicor AB is a two-side acrylic coated, sealable OPP film designed for general use in overwrap and horizontal packaging. It can be surface printed, reverse printed, or used unpri.. |
|||
Thickness | 33.0 microns | 1.30 mil | ExxonMobil Method |
ExxonMobil Bicor™ 32MB600 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, As.. |
|||
Thickness | 33.0 microns | 1.30 mil | ExxonMobil Method |
ExxonMobil Bicor™ 32MB768 OPP Film Product Description: A High gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side very low temperature seal (VTLS) coating. PVdC provides excellent moistu.. |
|||
Thickness | 33.0 microns | 1.30 mil | ExxonMobil Method |
ExxonMobil Bicor™ 32MB777 OPP Film Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated one side PVdC, one side acrylic. This film provides outstanding performance on all packaging machin.. |
|||
Thickness | 33.0 microns | 1.30 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 33LL247 OPP Film Product Description: A super white opaque, high gloss, caviated BOPP film designed for use in reel-fed warp-around labeling applications where superior graphics are desired.Availability: Africa & Mi.. |
|||
Thickness | 33.0 microns | 1.30 mil | ASTM D3652 |
3M 1614 Polyester Protective Tape 3M™ Polyester Protection Tape 1614 is a polyester tape with a low-tack adhesive system for temporary surface protection.Information provided by 3M |
|||
Thickness | 33.0 microns | 1.30 mil | ASTM D3652 |
3M 1675 Polyester Protective Tape 3M™ Polyester Protection Tape 1675 is a polyester tape with a low-tack adhesive system for temporary surface protection.Information provided by 3M |
|||
Thickness | 33.0 microns | 1.30 mil | Facestock |
3M 7744FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Thickness | 33.0 microns | 1.30 mil | Facestock |
3M 7745FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Film 7745FL utilizes a matte clear polyester that is recommended for optimum durability and appearance in dot matrix and hand writable applications. The matte coating r.. |
|||
Thickness | 33.0 microns | 1.30 mil | Carrier |
3M 9738 Double Coated Splicing Tape 3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres.. |
|||
Thickness | 33.0 microns | 1.30 mil | Carrier |
3M 9738R Double Coated Splicing Tape 3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres.. |
|||
Thickness | 33.0 microns | 1.30 mil | Faceside Adhesive |
3M 9824 Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Thickness | 33.0 microns | 1.30 mil | Backside Adhesive |
3M 9824 Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Thickness | 33.0 microns | 1.30 mil | Adhesive |
3M 7120 Performance Paper Label Material 3M™ Label Materials 7120 and 7122 latex impregnated paper with 3M™ 400 and 320 adhesives offer good conformability to curved surfaces and resistance to staining and moisture. Label Material 7120 h.. |
|||
Thickness | 33.0 microns | 1.30 mil | Facestock |
3M 7744 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Thickness | 33.0 microns | 1.30 mil | ExxonMobil |
ExxonMobil OPPalyte® 30 HM OPP Film Product Description: White opaque OPP film with a proprietary cavitated core. Designed for cold seal applications and is used as a surface print, monoweb, or as the inside web of a lamination. Avail.. |
|||
Thickness | 33.0 microns | 1.30 mil | ExxonMobil Method |
ExxonMobil Oppalyte™ 33ICE OPP Film Product Description: Coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal on.. |
|||
Thickness | 33.0 microns | 1.30 mil | ExxonMobil Method |
ExxonMobil Oppalyte™ 33MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |