Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 152 microns | 6.00 mil | Cured Ply |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, G30-700 Uni-Tape Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Thickness | 152 microns | 6.00 mil | side 1; Arlon SQA-TMS-003 |
Arlon A3020-B004-12 Silicone Rubber/Fiberglass Laminate
(discontinued **) Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film |
|||
Thickness | >= 152 microns | >= 6.00 mil | Side 1 |
Arlon 518581R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th.. |
|||
Thickness | 152 microns | 6.00 mil | ASTM D374 |
Dow Saran® 560 Vapor Retarder Film Saran™ Vapor Retarder Film is a biaxially oriented barrier film designed as a water vapor retarder for insulation applications. It is available in 600 gauge. Roll size: 35.5" x 250 long.Informat.. |
|||
Thickness | 152 microns | 6.00 mil | Side 1 |
Arlon 19576R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat.. |
|||
Thickness | 152 microns | 6.00 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 514B12R006 0.006" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2116 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Thickness | >= 152 microns | >= 6.00 mil | Side 1 |
Arlon 51583R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 152 microns | 6.00 mil | Side 2, Layer 1; Arlon SQA-TMS-003 |
Arlon 55148R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data r.. |
|||
Thickness | 152 microns | 6.00 mil | Side 2, Layer 2; Arlon SQA-TMS-003 |
Arlon 55148R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data r.. |
|||
Thickness | 152 microns | 6.00 mil | Liner |
3M 9671 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55578R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Appearance:.. |
|||
Thickness | 152 microns | 6.00 mil | Side 2, Layer 1; Arlon SQA-TMS-003 |
Arlon 55578R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Appearance:.. |
|||
Thickness | >= 152 microns | >= 6.00 mil | Side 1, Uncured Rubber Layer |
Arlon 55579R028M 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | >= 152 microns | >= 6.00 mil | Side 2 |
Arlon 55589W028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or.. |
|||
Thickness | 152 microns | 6.00 mil | side 1; Arlon SQA-TMS-003 |
Arlon 56976B026 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 152 microns | 6.00 mil | side 1; Arlon SQA-TMS-003 |
Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber |
|||
Thickness | 152 microns | 6.00 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 61089R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Denier Vectran HS Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 1000 Denier HS Appearance: Red silicone gum on fabricThis data represents t.. |
|||
Thickness | 152 microns | 6.00 mil | layer 2; Arlon SQA-TMS-003 |
Arlon R36319R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass |
|||
Thickness | 152 microns | 6.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon Thermabond® 48991A015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Thermabond® G2pr - electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 Fiberg.. |
|||
Thickness | 152 microns | 6.00 mil | Tape |
3M XR8115 Double Coated Paper Tapes 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of.. |
|||
Thickness | 152 microns | 6.00 mil | side 1, layer 2 uncured silicone; Arlon SQA-TMS-003 |
Arlon 51228R015 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51231R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51273R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: Polyethylene This data represents typical values for the production materia.. |
|||
Thickness | 152 microns | 6.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51273R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: Polyethylene This data represents typical values for the production materia.. |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51991A020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typica.. |
|||
Thickness | 152 microns | 6.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51991A020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typica.. |
|||
Thickness | >= 152 microns | >= 6.00 mil | Side 2 |
Arlon R33099G028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl.. |
|||
Thickness | 152 microns | 6.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon R38726R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured SiliconeThis data represents typical values for the production material. The.. |
|||
Thickness | 152 microns | 6.00 mil | ASTM D3652 |
3M Scotch® 894 Filament Tape Scotch® Tape 894 is a general-purpose packaging tape reinforced with continuous glass-yarn filaments that give the tape high tensile strength and low stretch. The clear 3M™ Scotchpro™ Film backin.. |
|||
Thickness | 152 microns | 6.00 mil | ASTM D3652 |
3M Scotch® 897 Filament Tape Scotch® Tape 897 is a glass-filament-reinforced tape suitable for light to medium duty strapping, bundling, reinforced applications. Scotch® Tape 897 has a synthetic rubber resin adhesive with goo.. |