Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 178 microns | 7.00 mil | Thermal Conductor Thickness |
Parker Chomerics T-Wing™ Heat Spreader Chomerics family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are not appropriate. T-Wing spreaders consist of.. |
|||
Thickness | 178 microns | 7.00 mil | Carrier; Arlon SQA-TMS-003 |
Arlon 31580R020 0.020" (0.508 mm) Uncured Silicone Rubber on HDPE Carrier
(discontinued **) Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: High Density PolyethyleneAppearance: Red silicone gum on polymer linerThis data represents typical values for the.. |
|||
Thickness | 178 microns | 7.00 mil | Nominal |
DuPont™ Nomex® 414 Paper, 7 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Thickness | 178 microns | 7.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 19146R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Black silicone gum and rubber on fiberglass clothT.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7052 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7045 and 7052 are durable, high performance materials that offer good durability and moisture resistance. These vinyl label stocks utilize 3M™.. |
|||
Thickness | 178 - 229 microns | 7.00 - 9.00 mil | Overall |
Arlon R34172W008 0.008" (0.203 mm) Cured, Unsupported Silicone Rubber on a Mylar Carrier Design/Construction:Side 1: Cured, Unsupported Silicone Rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FL015 Lexan Label Product 3M™ Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P1212, which is a high .. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FM015 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FP031105 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FV065 Semi-Rigid White Vinyl Label Product 3M™ Semi-Rigid White Vinyl Label Products are white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clarity general.. |
|||
Thickness | 178 microns | 7.00 mil | Facestock |
3M FVS14S Static Cling Label Materials 3M™ Static Cling Label Materials are highly plasticized vinyl label materials available in white or clear that adhere to most clean smooth surfaces such as glass, painted metal, and most smooth pla.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-10 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-14 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ IJ680-10 Reflective Graphic Film 6-mil flexible, enclosed lens, retroreflective films; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Pressure.. |
|||
Thickness | 178 microns | 7.00 mil | Backing; ASTM D1000 |
3M Scotch™ 2210 Vinyl Mastic Pads and Rolls 3M™ Scotch™ Brand 2200 Pads and 2210 Rolls are self fusing, rubber based insulating compounds laminated to a flexible, all weather grade vinyl (PVC) backing. These tape rolls and precut pads are d.. |
|||
Thickness | 178 microns | 7.00 mil | Total; ASTM D3752 |
3M 398FR Glass Cloth Tape 3M™ Glass Cloth Tape 398FR has an acrylic adhesive for many applications requiring high adhesion, an abrasion-resistant backing and flame retardant properties. This product is typically used for se.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7025 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7032 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7035 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7052W Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products are durable, high performance materials that offer good durability and moisture resistance. These vinyl label stocks utilize 3M™ Adhesive P140.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7053 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7046 and 7053 are durable, high performance materials that offer excellent durability and moisture resistance. These vinyl label stocks utilize.. |
|||
Thickness | 178 microns | 7.00 mil | Side 1 |
Arlon 51224R015P 0.015" Semi-cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassInterleave: 3 mil PolyethyleneThis data represents typical values for the production material and shou.. |
|||
Thickness | 178 microns | 7.00 mil | Side 1 |
Arlon 51344R015 0.015" (0.381 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-Cured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to .. |
|||
Thickness | 178 microns | 7.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55103R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber This data represents typical values for the production materia.. |
|||
Thickness | 178 microns | 7.00 mil | layer 2; Arlon SQA-TMS-003 |
Arlon 55109R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass |
|||
Thickness | 178 microns | 7.00 mil | Polyester |
3M 9061MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FM041909 White Polyester Label Products 3M™ White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive P1480, which .. |
|||
Thickness | 178 microns | 7.00 mil | with adhesive |
3M Scotchcal™ IJ65 Perforated Window Graphic Film Film IJ65 is an intermediate, 6-mil vinyl film with a 50% die-perforated pattern and a removable, pressure adhesive. This film allows a full image to be seen on the outside of a window while allowin.. |
|||
Thickness | 178 microns | 7.00 mil | |
Aremco Pyro-Tape™ 682-DS High Temperature Tape Double sided, single layer, fiberglass tape with silicone adhesive Applications Double Sided Features Assembly of high temp components and films. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FV016405 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |