Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 140 - 216 microns | 5.50 - 8.50 mil | Side 2 |
Arlon 19566R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The.. |
|||
Thickness | 140 - 216 microns | 5.50 - 8.50 mil | Side 2 |
Arlon 19576R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat.. |
|||
Thickness | 140 - 216 microns | 5.50 - 8.50 mil | Side 2 |
Arlon R34896R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 165 - 216 microns | 6.50 - 8.50 mil | Overall |
Arlon 47561R007 0.0075" (0.190 mm) Uncured Rubber Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not .. |
|||
Thickness | 165 - 216 microns | 6.50 - 8.50 mil | Overall |
Arlon 47576R007 0.0075" (0.190 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mate.. |
|||
Thickness | 140 - 216 microns | 5.50 - 8.50 mil | Side 1 |
Arlon 51970R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, or .. |
|||
Thickness | 165 - 216 microns | 6.50 - 8.50 mil | Overall |
Arlon 47573R007 0.0075" (0.190 mm) Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured RubberSide 2: Cured Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specifica.. |