Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 8.00 g/m²/day | 0.515 g/100 in²/day | At 38°C/90% RH; ISO 15106-2 |
Borealis Borstar® FB2230 LLDPE for Film Borstar BF2230 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from .. |
|||
Water Vapor Transmission | 8.00 g/m²/day | 0.515 g/100 in²/day | At 38°C/90% RH; ISO 15106-2 |
Borealis Borstar® FB4230 LLDPE for Film Borstar FB4250T is a high molecular weight linear low density polyethylene grade combining good extrusion properties, excellent draw properties and good mechanical strength. Film made from Borstar .. |
|||
Water Vapor Transmission | 8.00 g/m²/day | 0.515 g/100 in²/day | ASTM F372 |
Eastman Sahara Film Sahara Films are developed for use in applications where increased temperature resistance is desired.Applications/UsesHigh temperature printable films |
|||
Water Vapor Transmission | 8.00 g/m²/day | 0.515 g/100 in²/day | Cast Film at 2.0 mil; ASTM F-1249 |
Chevron Phillips MarFlex® 2121 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for cast film applications that require: Good processabilityGood drawdownEdge tear resistanceLow neck-in Applications: Typical cast film applicatio.. |
|||
Water Vapor Transmission | 8.00 g/m²/day | 0.515 g/100 in²/day | ASTM E96 Procedure E |
DuPont Teijin Films Mylar® M33 Polyester Film, 50 Gauge, PVDC Coated Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. the coating is heat sealable, and is an excellent moisture and.. |
|||
Water Vapor Transmission | 8.00 g/m²/day | 0.515 g/100 in²/day | 23°C/85%r.h.; DIS 15106-1/-2 |
EMS-Grivory Grivory® L 25 G nat 6011 PA12 Product Description: Grilamid L 25 G natural 6011 is a high viscosity, lubricated polyamide 12. This product has the following features: Very tastelessHigh toughness, even at low temperaturesGood re.. |
|||
Water Vapor Transmission | 8.00 g/m²/day | 0.515 g/100 in²/day | ASTM E96 Procedure E |
DuPont Teijin Films Mylar® M30 Polyester Film, 50 Gauge (14 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and.. |
|||
Water Vapor Transmission | 8.00 g/m²/day | 0.515 g/100 in²/day | ASTM E96 Procedure E |
DuPont Teijin Films Mylar® M30 Polyester Film, 75 Gauge (21 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and.. |
|||
Water Vapor Transmission | 8.00 g/m²/day | 0.515 g/100 in²/day | ASTM E96 Procedure E |
DuPont Teijin Films Mylar® M30 Polyester Film, 100 Gauge (25 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and.. |
|||
Water Vapor Transmission | 8.00 g/m²/day | 0.515 g/100 in²/day | 23°C/85%r.h.; DIS 15106-1/-2 |
EMS-Grivory Grivory® L 25 nat PA12 Product Description: Grilamid L 25 is a high viscosity polyamide 12. This product has the following features: Very tasteless High toughness, even at low temperatures Good resistance to weathering Go.. |