Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 10.86 g/m²/day | 0.6994 g/100 in²/day | E 96/66 |
Total Finathene® HL 328 HDPE resin
(discontinued **) Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by .. |