Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 52.0 g/m²/day @Temperature 38.0 °C |
3.35 g/100 in²/day @Temperature 100 °F |
90% RH; 1 µm |
Solvay Specialty Polymers Diofan® P530 Polyvinylidene Chloride (PVDC)
(discontinued **) DIOFAN® P530 is an one-component latex, water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. Developed.. |