Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 230 cc/m²/day | 14.8 cc/100 in²/day | 25°C, 1.0 µm, 0% RH |
Solvay Specialty Polymers Diofan® P530 Polyvinylidene Chloride (PVDC)
(discontinued **) DIOFAN® P530 is an one-component latex, water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. Developed.. |